Supplying dimension

Round bar from         30mm to 600mm Diameter

Flat and square bar from  30mm to 500mm Width

8mm to 300mm Thickness

*accept special shape

 

Forming option

Hot rolling or hot forged

 

Smelting process

EAF →VD→LF→ESR Electro-Slag Remelting

 

Surface option

Black

Grinding

Rough turned

Peeled

Polished

 

Quality

UT, size and surface for each pcs

Macrostructure

Ferritic Metallographic

Grain size

Nonmetallic inclusion

Etch test of tower sample

 

Delivery condition and hardness

Annealed or high temperature temper

Annealed high temperature temper Hardness
800 to 900 Celsius, slow 700 to 770 Celsius, fast Max 200 HBW

*Accept +QT delivery condition

 

Equivalent Grade

Chinese UNS Chinese New Grade Chinese Old Grade JIS ASTM SAE AISI EN BS DIN EN BS DIN
S41010 12Cr13 1Cr13 SUS410 410 1.4006 X12Cr13

 

Chemical component

C Si Mn P S Ni Cr Cu
0.10 to 0.15 Max 0.60 Max 0.60 Max 0.030 Max 0.020 Max 0.60 11.50 to 13.50 Max 0.30

 

Mechanical property and heat treatment

Quench temperature Temper temperature Specified Plastic Elongation Strength Tensile strength Elongation Reduction Impact Hardness
980 to 1040 Celsius, oil 660 to 770 Celsius, air Min 440 Mpa Min 620 Mpa Min 20 % Min 60% Min 35 KJ 192 to 241 HBW

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Get A Free Quote!

Fushun TEL: +86-731-89903933

Fushun FAX: +86-731-89853933

General Manager: Ms. Florence Tang

Whatsapp/Phone/WeChat:+86-13319591838

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : info@fushunspecialsteel.com

Whatsapp:+86-18692275455

x