Work rolls, back-up rolls and intermediate rolls for hot and cold strip mills. Supplied as forged and rehardened, with the hardened shell depth, the core toughness and the journal dimensions agreed against the mill stand rather than against a general table.
Parts we forge
- Back-up Roll Forgings
- Intermediate Roll Forgings
- Leveller & Skin-Pass Roll Forgings
- Cold Mill Work Roll Forgings
Send the drawing with the finished weight, the material specification and the testing level. We quote the ingot route, the forging ratio, the heat treatment cycle and the non-destructive testing schedule — then certify the part, not a separately melted test bar.