manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

34CrNiMo6 SNCM439 35NCD6 EN24 817M40 1.6582 Alloy Steel

Grade reference · Cross-reference · 34CrNiMo6

34CrNiMo6 Equivalent Grades and Chemical Composition

A cross-reference page, not a stock list. If you are checking whether 1.6582, EN24, 817M40, SNCM439 or 34CrNiMo6 will substitute for each other, the answer is on this page. If you need to buy the steel, the supply page is linked below.

6 designations
One steel
0.30–0.38 C
Base chemistry
Ni-Cr-Mo
Family
Table below
Equivalents
Download datasheet (PDF)One page: designation, chemistry, mechanical properties, supply range and inspection scope.

Read this first

This page exists to answer one question: is grade X the same as grade Y. It is a reference table, not an offer. The commercial page with sizes, delivery conditions and certification is the 1.6582 / 34CrNiMo6 supply page.

Keeping the two separate matters. A buyer searching “34crnimo6 equivalent” wants a table in ten seconds. A buyer searching “34crnimo6 supplier” wants sizes and a certificate. One page trying to do both ranks for neither.

The six designations, side by side

System Designation Standard C Ni Cr Mo
EN / DIN 34CrNiMo6 / 1.6582 EN 10083-3 0.30–0.38 1.30–1.70 1.30–1.70 0.15–0.30
British EN24 / 817M40 BS 970 0.36–0.44 1.30–1.70 1.00–1.40 0.20–0.35
AISI / SAE 4337 ASTM A29 0.30–0.37 1.65–2.00 0.70–0.90 0.20–0.30
Japanese SNCM439 JIS G4105 0.36–0.43 1.60–2.00 0.60–1.00 0.15–0.30
French 35NCD6 AFNOR 0.32–0.40 1.60–2.00 0.90–1.20 0.15–0.30
Russian 38Ch2N2MA GOST 0.35–0.42 1.30–1.70 1.30–1.70 0.15–0.25

They are close, not identical. Carbon and nickel spread by up to 0.08 and 0.70 % across the six, which changes hardenability and the tempering response.

Where the substitutions actually bite

Hardenability is the first difference. 4337 with 1.65–2.00 % nickel hardens deeper than 1.6582 with 1.30–1.70 %. In a 150 mm section that shows up as a lower core hardness after the same quench, and a tensile test taken at the quarter point can fail even though the surface is correct.

The second is tempering response. The British 817M40 window runs higher carbon and lower chromium than 1.6582, so at the same tempering temperature it lands a few HRC harder. If the drawing specifies 850–1000 MPa in the T condition, a straight substitution without adjusting the temper will overshoot.

The third is residual control. EN 10083-3 caps phosphorus at 0.025 % and sulphur at 0.035 %; JIS G4105 allows 0.030 and 0.030. On a part that will see impact loading, that difference in cleanliness is worth more than the price difference between the two.

If you are buying, go here

What you need Page
1.6582 / 34CrNiMo6 bar, sizes and certification 1.6582 / 34CrNiMo6 supply page
EN24 / 817M40 to BS 970 in the T condition EN24 and EN24T page
42CrMo4 / 1.7225, the lower-alloy alternative 42CrMo4 / 1.7225 page
AISI 4340, for sections above 250 mm AISI 4340 / 1.6511 page

Request a quote

Send these five lines and we quote within one working day
  • Which designation your drawing calls for, and which standard governs
  • Section size — the ruling section decides whether the substitution is safe
  • Required tensile or hardness window in the final condition
  • Quantity in pieces or kilograms
  • Certificate and inspection requirements

Email [email protected]  or use the form below. Drawings in DXF, STEP or PDF are all fine.

Related grades

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x