1. 1.5815 Description

Alloy special steel 35NiCr6 grade steel belongs to alloy steels for quenching and tempering. The material no. is 1.5815.

2. 1.5815 Application

Steel for heat improvement characterized by high strength properties, good ductility, resistance to fatigue and impact. Used for heavy-duty parts of engines, devices and machines, used in the production of crankshafts, gears, shafts, piston rods, bolts, heat-treated gears and piston rods.

• Crankshafts.
• Shafts.
• Various gears.
• Fasteners etc

3.All Grades Comparison

DIN EN ANFOR AECMA
1.5815 35NiCr6 35NC6 FE-PL62

3.Quality Standard

EN 10083 Steels for quenching and tempering. Technical delivery conditions for alloy steels
EN 10250 Open steel die forgings for general engineering purposes. Alloy special steels

4. 1.5815 Chemical Composition(%)

C Mn Si P S Cr Ni
0.30-0.37 0.60-0.90 0.40 max 0.025 max 0.025 max 0.80-1.10 1.20-1.60

5.Mechanical Properties(T=20°C if not differently stated)

Process Diameter(mm) Tensile Strength Rm (Mpa) Yield Strength Rp0.2 (Mpa) Elongation A5 (%) Area Reduction Ratio C (%) Impact Value Kv (J) Room Temperature Hardness (HB)
SOFT ANNEALED / / / / / / 223 max
QUENCHED AND TEMPERED 16 max 880-1080 740 min 12 min 40 min / 261-318
QUENCHED AND TEMPERED 16-40 880-1080 740 min 12 min 40 min 35 min 261-318
QUENCHED AND TEMPERED 40-100 780-980 640 min 15 min 40 min 35 min 231-289
[/custom_table]

6.HEAT TREATMENT:

Process TEMPERATURE °C Cooling Medium
Hot plastic deformation 850-1100 /
Normalization 850-880 air
Soft annealing 640-690 air
Hardening 840-860 oil
Tempering 530-630 air

7.Mill′s test certificate:

EN 10204/3.1 with all relevant data reg. chem. composition, mech. properties and results of testing.

In the above-mentioned grades we deliver:

Other indications of grades and substitutes:

AISI 3140, SNC1, SNC236, 640M40, EN111, 35NC5, 35NC6, 35 NC 6, 30NC6, 30 NC 6, 1.5710, 1.5815, 36NICR6, 36 NICR 6, 35NICR6, 35 NICR 6, 36 NICR 6-4, 36NICR6-4, 35NI5CR2, CSN 16240, 40NICR6, 40 NICR 6, 1.5711.

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

info@fushunspecialsteel.com

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : info@fushunspecialsteel.com

x