The URL of this page carries an old mistake. 1.8519 is 31CrMoV9, a nitriding steel — a different alloy with a different
application. 51CrV4 / 50CrV4 / 6150 / EN47 / 735A50 is a chromium-vanadium spring steel to EN 10089-2, and that is what
this page is about. If you reached this page looking for 1.8519, the
31CrMoV9 / 1.8519 page is the correct one.
51CrV4 BS970 EN47 735A50 735A51 DIN 1.8519 EN 50CrV4 6150 Spring Steels
1 51CrV4 Introduction:
The 6150 Spring Steels receive their special characteristics through quenching and tempering.
The processors need to make sure that their calculation method, design technique and processing procedure are aligned with the material. Precise temperature control is crucial for the part’s characteristics.
Therefore, the temperature needs to be adjusted according to the respective purpose of the material.
2 51CrV4 Applications:
Used widely in the motor vehicle industry AISI 6150 spring steels is suitable for many general engineering applications that require high tensile strength and toughness. Typical applications include crankshafts, steering knuckles, spindles, pumps and gears.
3 Quality Standard:
BS EN 10089 2002 Hot rolled steels for quenched and tempered springs
BS 970 part3 Specification for Wrought steels for mechanical and allied engineering purposes
4 All Grades Comparison:
| Material No. | EN | BS | JIS | ANFOR | UNE | GOST |
|---|---|---|---|---|---|---|
| 1.8519 | 50CrV4 | 735A51, 735M50, EN47 | SUP 10 | 50CrV4, 51CV4 | F1430 | 50HFA |
5 51CrV4 Chemical Composition(%)
| Steel Grade | C | Si | Mn | P | S | Cr | V |
|---|---|---|---|---|---|---|---|
| 6150 | 0.48-0.53 | 0.15-0.35 | 0.70-0.90 | 0.035 max | 0.040 max | 0.90-1.10 | 0.15 min |
| SUP10 | 0.47-0.55 | 0.15-0.35 | 0.65-0.95 | 0.030 max | 0.030 max | 0.80-1.10 | 0.15-0.25 |
| 51CrV4 | 0.47-0.55 | 0.40 max | 0.70-1.10 | 0.025 max | 0.025 max | 0.90-1.20 | 0.10-0.25 |
| 735A50 | 0.46-0.54 | 0.10-0.40 | 0.60-0.90 | 0.040 max | 0.040 max | 0.80-1.10 | 0.15 min |
6 HEAT TREATMENT:
- FORGING: Preheat carefully, then raise temperature to 1050°C for forging. Do not forge below 840°C. After forging cool slowly in a furnace.
- ANNEALING: Heat slowly to 820-840°C, soak well and cool slowly in a furnace.
- HARDENING: Heat slowly to 650-700°C and thoroughly soak. Continue to heat the 6150 steel to the final hardening temperature of 830-860°C and allow to be heated through. Oil quench.
- TEMPERING: Temper 6150 spring steel immediately after hardening whilst tools are still hand warm. Re-heat to the tempering temperature then soak for one hour per 25 millimetre of total thickness (2 hours minimum) Cool in air. Tempering of this grade will be between 400-600°C for most applications.
7 Mill′s test certificate:
EN 10204/3.1 with all relevant data reg. chem. composition, mech. properties and results of testing.