102Cr6 1.2067 ШХ15 Cold Work Tool Steel

102Cr6 1.2067 ШХ15 Cold Work Tool Steel

102Cr6 1.2067 ШХ15 Cold Work Tool Steel

Grade :     102Cr6    Number:     1.2067

 

Classification:     Alloy cold-work tool steel

 

Standard

EN 10132-4: 2000 Cold rolled narrow steel strip for heat treatment. Technical delivery conditions. Spring steels and other applications

EN ISO 4957: 2000 Tool steels

 

102Cr6 as a differently graded flat or round grade is used for the manufacture of cold forming dies and stamps, file cutters, wood and paper cutting knives, taps, scrapers, or broaches.

We can provide more services:

1、Hardening and tempering
2、Vacuum heat treatment
3、Polished bright surface
4、Milling bright surface
5、CNC machine
6、Deep drilling
7、Cut into small pieces
8、Make it closer to the mold
Welcome to inquiry price from drawing

PRODUCT DESCRIPTION

The alloy is usually produced by EAF /VD /LF followed by electroslag refining (ESR) if necessary for special purpose.

Bars and, where applicable, forgings are subjected to ultrasonic examination based on the different level according to the buyers’ requirements.

Bars are usually supplied bright in the softened condition.

Final heat treatment – heat treatment / QT

Cutting:

Precision cutting to standard dimensions

Custom cutting according to client specifications

Cold Work Tool Steel Dimensions

We offer premium cold work tool steel in various forms, manufactured with advanced 5000-ton forging press technology for superior density and performance.

Product Form Specifications
Forged Round Bar Dia. up to 1200mm
Forged Flat Bar Thickness 100-600mm, Width 300-2000mm
Rolled Round Bar Dia. 10-200mm
Hot Rolled Plate Thickness 1-100mm, Width 60-1600mm

 

Composition Alloy constituents [%]

C: 0.95 – 1.10

Si: 0.15 – 0.35

Mn: 0.20 – 0.40

P: ≤ 0.025

S: ≤ 0.025

Cr: 1.35 – 1.60

Mo: ≤ 0.10

Ni: ≤ 0.40

 

Heat treatment of 102Cr6, 1.2067 steel:

Softening annealing at 780 – 810 ℃ with furnace cooling to 550 – 600 ℃ at 10-20 ℃ hourly with subsequent air or isothermal cooling at 680 – 720 ℃ Tempering at 830 – 870 ℃ with cooling in oil or water at 820 – 850 ℃ Tempering at 150 – 170 ℃ in the air

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x