105V 1.2834 Alloy Cold Work Tool Steel

105V 1.2834 Alloy Cold Work Tool Steel

105V 1.2834 Alloy Cold Work Tool Steel

Grade :105V

Number:1.2834

Classification: Alloy cold-work tool steel

Standard: EN ISO 4957: 2000 Tool steels

Cutting:

Precision cutting to standard dimensions

Custom cutting according to client specifications

Cold Work Tool Steel Dimensions

We offer premium cold work tool steel in various forms, manufactured with advanced 5000-ton forging press technology for superior density and performance.

Product Form Specifications
Forged Round Bar Dia. up to 1200mm
Forged Flat Bar Thickness 100-600mm, Width 300-2000mm
Rolled Round Bar Dia. 10-200mm
Hot Rolled Plate Thickness 1-100mm, Width 60-1600mm

 

Our capacity :

Delivery condition : Normalized, or Annealed, or Quenched and Tempered ;

Surface condition : Grounded, or Turned, or Polished

 

Our advantage :

  1. High Quality, Reasonable Price
  2. Over 40 Years Experience
  3. ISO NQA Certificated Factory
  4. Worldwide shipping
  5. Emergency Orders and Fast Delivery

 

Equivalent grades of steel 105V (1.2834)

EU Japan
EN JIS
105V SKS43

 

Chemical composition %  of steel 105V (1.2834):  EN 4957-2000

C Si Mn P S V
1 – 1.1 0.1 – 0.3 0.1 – 0.4 max   0.03 max   0.03 0.1 – 0.2

 

Hardening of steel 105V (1.2834):  EN 4957-2000

Hardness (annealed) b +A HBW max. Hardening test
Austenitizing temperature °C (±10 °C) Quenching medium Tempering temperature °C (±10 °C) Hardness HRC min.
212 790 w 180 61

 

Surface condition

Usual surface conditions are

  1. a) the hot-rolled or forged condition (= as hot worked),
  2. b) the machined (ground, polished, turned, peeled or milled) condition, and
  3. c) the cold-reduced condition.

Unless otherwise agreed at the time of enquiry and order, the products shall be delivered in the surface condition hot worked.

 

Mill′s test certificate

EN 10204/3.1 with all relevant data reg. chem. composition, mech. properties and results of testing.

 

Smelting Option

1 EAF: Electric Arc Furnace

2 EAF+LF+VD: Refined-smelting and vacuum degassing

3 EAF+ESR: Electro Slag Remelting

4 EAF+PESR: protective atmosphere Electro Slag Remelting

5 VIM+PESR: Vacuum induction melting

 

Forming Option

1 Hot rolling process

2 Hot Forging: Electro-hydraulic; High-speed-hydraulic; Oil-hydraulic; Precision-forging

 

Heat-treatment Option

1 +A: Annealed (full/soft/spheroidizing)

2 +N: Normalized

3 +NT: Normalized and tempered

4 +QT: Quenched and tempered (water/oil)

 

Surface Option

1 Black Surface

2 Grounded: Bright but rough ; Not precision

3 Machining for plate: Bright and precision; Little turning scar

4 Peeled/Turned: Bright and precision; Little turning scar

5 Polished: Very Bright and precision size; Not turning scar

 

Other Services

1 Cutting: Small pieces

2 CNC Machine: Produce as your drawing

3 Package: Bare/Nylon/Canvas/Wooden

4 Payment:T/T, L/C, O/A(request credit)

5 Transport:FOB/CFR/CIF/DDU/DDP (train/ship/Air)

 

We also supply :

1.2510/H10, 1.2842, 1.2379/D2, 1.2080/X210Cr12/D3, 1.2436, 1.2365, 1.2885, 1.2343, 1.2344/H13/SKD61, 1.2581/H21, 1.2709, 1.2345, 1.2738/P20NI, 1.2083/420J2, 1.2316, 1.2312/P20S, 1.2311, 1.2764

For all products, please check here: Fushun products

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x