1.4104 X14CrMoS17 Martensitic Stainless Steel

1.4104 X14CrMoS17 Martensitic Stainless Steel

1.4104 X14CrMoS17 Martensitic Stainless Steel

Our supply size:

Diameter : 80 to 600 mm ;

Length : 1000 to 9000 mm ;

 

Our advantage:

  1. High Quality, Reasonable Price
  2. Over 40 Years Experience
  3. ISO NQA Certificated Factory
  4. Worldwide shipping
  5. Emergency Orders and Fast Delivery

 

Introduce

1.4104 is a rust- and acid-resistant martensitic chromium steel with added sulfur, which improves its machinability. However, despite the high chromium content, the corrosion resistance is reduced due to the sulfur.

 

Chemical composition % of steel X14CrMoS17 (1.4104): EN 10088-3-2005

C Si Mn P S Cr Mo
0.1 – 0.17 max   1 max   1.5 max   0.04 0.15 – 0.35 15.5 – 17.5 0.2 – 0.6

 

Mechanical properties of steel X14CrMoS17 (1.4104)

Rm – Tensile strength (MPa) (+QT650) 650-850
Rp0.2 0.2% proof strength (MPa) +QT650 500
A – Min. elongation at fracture (%) (+QT650) 44846
  Brinell hardness   (HB):   (+A) 220

 

Application

1.4104 stainless steel is a martensitic stainless steel grade which can be heat threated. This grade is written as 1.4104 or X14CrMoS17 according to EN norm and it is written as UNS S43020 according to UNS norm. 1.4104 material is commenly mixed up with 430F grade stainless steel. There is only a small carbon percantage difference between 430F and 1.4104 grade and the main difference is that 1.4104 grade can be heat threated, but 1.4105 (430F) can not be heat threated. Because of this similarity, most of the people know this grade as 430F (1.4104), but this is a mistake. 1.4104 grade does not have any equivalent in AISI norm. (Like 304 or 316 or 430F) So this is the biggest reason wht 430F and 1.4104 is commenly mixed. 1.4104 grade includes good amouth of sulfur and this sulfur makes the machinability of this grade easy. 1.4104 material carbon content level is good enough for heat threatment and 1.4104 grade materials can be heat threated. 1.4104 material usually used in pump parts and automative parts. Since 1.4105 (AISI 430F) and 1.4104 grade are really similar, in many applications both of these stainless grades can be used alternative to each other.

 

Smelting Option

1 EAF: Electric Arc Furnace

2 EAF+LF+VD: Refined-smelting and vacuum degassing

3 EAF+ESR: Electro Slag Remelting

4 EAF+PESR: protective atmosphere Electro Slag Remelting

5 VIM+PESR: Vacuum induction melting

 

Forming Option

1 Hot rolling process

2 Hot Forging: Electro-hydraulic; High-speed-hydraulic; Oil-hydraulic; Precision-forging

 

Heat-treatment Option

1 +A: Annealed (full/soft/spheroidizing)

2 +N: Normalized

3 +NT: Normalized and tempered

4 +QT: Quenched and tempered (water/oil)

 

Surface Option

1 Black Surface

2 Grounded: Bright but rough ; Not precision

3 Machining for plate: Bright and precision; Little turning scar

4 Peeled/Turned: Bright and precision; Little turning scar

5 Polished: Very Bright and precision size; Not turning scar

 

Other Services

1 Cutting: Small pieces

2 CNC Machine: Produce as your drawing

3 Package: Bare/Nylon/Canvas/Wooden

4 Payment:T/T, L/C, O/A(request credit)

5 Transport:FOB/CFR/CIF/DDU/DDP (train/ship/Air)

 

Mill test certificate

EN 10204/3.1 with all relevant data reg. chem. composition, mech. properties and results of testing.

 

We also supply :

1.2510/H10, 1.2842, 1.2379/D2, 1.2080/X210Cr12/D3, 1.2436, 1.2365, 1.2885, 1.2343, 1.2344/H13/SKD61, 1.2581/H21, 1.2709, 1.2345, 1.2738/P20NI, 1.2083/420J2, 1.2316, 1.2312/P20S, 1.2311, 1.2764

For all products, please check here: Fushun products

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x