What Is M42 Tool Steel?

What Is M42 Tool Steel?

 

Introduction

Molybdenum high-speed steels and tungsten high-speed steels are two types of high-speed tool steels. Molybdenum high-speed steels, also known as group M steels, comprise less initial cost. Molybdenum steel types M1 to M10 have tungsten whereas cobalt is not found in type M6. Cobalt is totally absent in these types of molybdenum high-speed steels.

 

M42 tool steel, a type of molybdenum high speed tool steel, has good wear resistance and hot hardness along with high hardness values.

 

Chemical Composition

The chemical composition of M42 molybdenum high speed tool steel is outlined in the following table.

Element Content (%)
C 1.05-1.15
Mn 0.15-0.40
Si 0.15-0.65
Cr 3.50-4.25
Ni 0.3
Mo 9.00-10.00
W 1.15-1.85
V 0.95-1.35
Co 7.75-8.75
Cu 0.25
P 0.03
S 0.03

 

Physical Properties

Physical Properties Metric Imperial
Density 7.81 g/cm3 0.282 lb/in3

 

Mechanical Properties

Mechanical Properties Metric Imperial
Hardness, Rockwell C (oil quenched from 1204°C, 5 minutes) 64.3 64.3
Hardness, Rockwell C (oil quenched from 1177°C, 5 minutes) 65.5 65.5
Hardness, Rockwell C(oil quenched from 1163°C) 65.8 65.8
Izod impact unnotched (oil quenched at 1191°C; 510°C temper temperature) 13.6 J 10.0 ft- lb
Izod impact unnotched (oil quenched at 1191°C; 622°C temper temperature) 24.4 J 24.4 J
Machinability (1% carbon steel) 35.0 – 40.0% 35.0 – 40.0%
Poisson’s ratio 0.27-0.30 0.27-0.30
Elastic modulus 190-210 GPa 27557-30457 ksi

 

Other Designations

Analyze Your Metals | Request a Quote

Equivalent materials to M42 molybdenum high speed tool steel are:

 

AFNOR 07-05-04-04-02

DIN 1.3246

ASTM A600

FED QQ-T-590

UNS T11342

DIN 1.3247

Fabrication and Heat Treatment

Machinability

M42 tool steel can be drilled, turned, threaded, broached, milled and tapped when it is in its annealed condition and rated at 45% of 1% carbon steel.

 

Forging

M42 molybdenum high speed tool steel is preheated to 871°C (1599°F) in a slow manner and then soaked. This is followed by rapid heating to 1093°C (1999°F) and slow cooling. Temperatures below 982°C (1799°F) are not suitable for the forging process.

 

Tempering

M42 tool steel is tempered for three times at 538-593°C (1000-1099°F) and then cooled completely between cycles to obtain good results. Tempering is performed in vacuum furnaces or in salt baths.

 

Annealing

M42 tool steel is heated at 871°C (1599°F) and then cooled slowly in a furnace.

 

Hardening

M42 tool steel is preheated to 871°C (1599°F), soaked and finally heated to 1204°C (2199°F).

 

Quenching

A salt media is used for quenching M42 tool steel at 538°C (1000°F) and then the steel is air cooled.

 

Applications

M42 tool steel is mostly used for machine materials and super alloys that are difficult to machine. The machine materials include chasers, broaches, form and gear cutters, hobs, drills, milling cutters, end mills and taps.

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.