manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

N850 Nonmagnetic Steel

N850 Nonmagnetic Steel

N850 Nonmagnetic Steel

N850 Nonmagnetic Steel

We produce N850, Hastelloy C-22HS, non-mag material Steel Bars and Non Magnetic Hollow Bars.

 

1. CHEMICAL COMPOSITION

N850 is a special nonmagnetic, nickel chromium molybdenum alloy.

C Cr Mo Fe Co Ni
max. 0,01 20,00 – 22,00 15,00 – 18,00 max. 2,0 max. 1,0 remainder

 

2. MECHANICAL PROPERTIES

Following mechanical properties (tested at room temperature) are achieved by a special cold-working process over the full length of the collar:

TEXT OD KSI N/MM
Yield Strength (min.) 0,2%-offset method: OD up to 10“ 150 ksi 1035 N/mm²
Tensile Strength (min.): 160 ksi 1104 N/mm²
Elongation (min.): 15% 15%
Reduction of area (min.): 50% 50%
Impact energy (min.): 100 ft.lb 135 J
Endurance Strength / N=10⁵ (min.): ± 90 ksi ± 620 N/mm²
Hardness Brinell: (min.): 300-430 HB 300-430 HB

 

3. MAGNETIC PROPERTIES

Relative permeability: ≤ 1,005.

 

4. CORROSION RESISTANCE

Superior corrosion properties compared to other Ni-based alloys are given.
The material specified conforms to ANSI/NACE MR0175 / ISO 15156.
This alloy can be used in environments containing 1000 psia (7000 kPa) H2S at a chloride concentration of 180000 mg/L and any in situ pH up to 550°F (288°C). It can be used also in environments containing 500 psia (3500 kPa) H2S at a chloride concentration of 180000 mg/L, at any situ pH and in the presence of elemental sulfur up to 400°F (204° C)

 

5. NON-DESTRUCTIVE TESTING

  • Magnetic inspection:Drill collars are 100% tested by a proprietary probe-testing process.
  • Ultrasonic inspection: Each collar is ultrasonically inspected over 100% of the volume according to ASTM E 114, last edition as a minimum level.

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.