manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

34CrNi3Mo Alloy Steel

34CrNi3Mo Alloy Steel

a high-strength alloy structural steel.

It is a commonly used large-scale steam turbine forging low-pressure rotor steel with good comprehensive mechanical properties and process properties. It has been widely used in the production of engine rotor and turbine impellers.

<<DATA SHEET 34CrNi3Mo Alloy Steel FUSHUN>>

Features and applications:

34CrNi3Mo is a high-strength alloy structural steel, is widely used in large-scale steam turbine forging low-pressure rotor steel, has good mechanical properties and process performance, has been widely used in engine rotor and steam turbine impeller production.

Steel performance, use and 30Cr2Ni2Mo similar. Material welding performance is poor, prone to cold cracking after welding.

 

Chemical Composition:

C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Mo(%) Cu(%)
0.30~0.40 0.17 ~ 0.37 0.50 ~ 0.80 ≤0.035 ≤0.035 0.70~1.10 2.75 ~ 3.25 0.25 ~ 0.40 ≤0.20

 

Mechanical Propoerties:

Yield Strength
Rp0.2(MPa)
Tensile Strength
Rm(MPa)
Elongation δ5 (%): Reduction
of area ψ (%):
Impact energy
Akv (J):
Impact toughness
value αkv (J/cm2)
Hardness
≥ 785(85) ≥ 900(85) ≥ 12 ≥ 40 ≥ 58 ≥ 55(5) ≥ 248 HB

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

info@fushunspecialsteel.com

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : info@fushunspecialsteel.com

x