manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

Die-casting Mould Tool Steel

Die-casting Mould Tool Steel

Die-casting Mould Tool Steel

Fushun are main manufacturer of tool steel for Die-casting Mould.

 

What is Die-casting Mould?

Die-casting moulds (for aluminum, copper alloys, etc.) are sophisticated tooling systems designed for producing metal components by injecting molten metal into precisely engineered cavities under high pressure. These moulds incorporate complex cooling channels, venting systems, and ejection mechanisms, along with carefully designed gates and runners to control metal flow. The mould assembly must maintain dimensional stability while repeatedly handling high-temperature molten metal and rapid cooling cycles.

 

The primary function of die-casting moulds is to produce high-precision components with excellent surface finish and dimensional accuracy. They are extensively used in automotive, electronics, and consumer goods industries to manufacture complex parts like engine components, housing units, and structural elements. This process offers advantages including high production rates, excellent detail reproduction, thin wall capabilities, and minimal post-processing requirements. Die-casting moulds can produce parts with complex geometries while maintaining tight tolerances and consistent quality.

 

The mould materials used in die-casting applications require specific alloying elements to withstand thermal fatigue and erosion from molten metal flow. Premium grade hot-work tool steels are used, containing carefully balanced combinations of chromium, tungsten, molybdenum, and vanadium to provide optimal thermal and mechanical properties. These materials offer excellent hot hardness, thermal shock resistance, and resistance to heat checking. The microstructure features thermally stable carbides that maintain hardness and wear resistance under repeated thermal cycling. Special surface treatments and coatings are often applied to enhance thermal fatigue resistance and prevent soldering of cast metal to the mould surface, while sophisticated heat treatment processes ensure optimal performance under extreme temperature conditions.

Die-casting Mould Materials

—     — 4Cr5W2VSi
H21 SKD5 1.2581 X30WCrV9-3 3Cr2W8V
H11 SKD6 1.2343 X37CrMoV5-1 4Cr5MoSiV
H13 SKD61 1.2344 X40CrMoV5-1 4Cr5MoSiV1
H10 — 1.2365 — 4Cr3Mo3SiV
H12 — 1.2605 X35CrWMoV5 4Cr5MoWVSi
— —   — 3Cr3Mo3W2V
      — 4Cr5Mo2V
— SKD7   32CrMoV12-28 3Cr3Mo3V
— —   — 4Cr5Mo3V
—       3Cr3Mo3VCo3
— —   — 00Ni18Co8Mo5TiAl
        Ni53Cr19Mo3TiNb

 

Chemical Composition of Die-casting Mould

Grade C Si Mn Cr W Mo Ni V
4Cr5W2VSi 0.32~0.42 0.80~1.20 ≤0.40 4.50~5.50 1.60~2.40     0.60~1.00
3Cr2W8V 0.30~0.40 ≤0.40 ≤0.40 2.20~2.70 7.50~9.00     0.20~0.50
4Cr5MoSiV 0.33~0.43 0.80~1.20 0.20~0.50 4.75~5.50 一 1.10~1.60    0.30~0.60
4Cr5MoSiV1 0.32~0.45 0.80~1.20 0.20~0.50 4.75~5.50   1.10~1.75   0.80~1.20
4Cr3Mo3SiV 0.35~0.45 0.80~1.20 0.25~0.70 3.00~3.75   2.00~3.00   0.25~0.75
4Cr5MoWVSi 0.32~0.40 0..80~1.20 0.20~0.50 4.75~5.50 1.10~1.60 1.25~1.60    0.20~0.50
3Cr3Mo3W2V 0.32~0.42 0.60~0.90 ≤0.65 2.80~3.30 1.20~1.80 2.50~3.00   0.80~1.20
4Cr5Mo2V 0.35~0.42 0.25~0.50 0.40~0.60 5.00~5.50   2.30~2.60   0.60~0.80
3Cr3Mo3V 0.28~0.35 0.10~0.40 0.15~0.45 2.70~3.20   2.50~3.00   0.40~0.70
4Cr5Mo3V 0.35~0.40 0.30~0.50 0.30~0.50 4.80~5.20    2.70~3.20 一 0.40~0.60
3Cr3Mo3VCo3 0.28~0.35 0.10~0.40 0.15~0.45 2.70~3.20   2.60~3.00   0.40~0.70
00Ni18Co8Mo5TiAl ≤0.03 ≤0.10 ≤0.15 ≤0.60   4..50~5.00 17.5~18.5  
Ni53Cr19Mo3TiNb ≤0.08 ≤0.35 ≤0.35 17.00~21.00   2.80~3.30 50.00~55.00  

 

Properties of Die-casting Mould Steel

Grade Annealed HBW
4Cr5W2VSi ≤229
3Cr2W8V ≤255
4Cr5MoSiV ≤229
4Cr5MoSiV1 ≤229
4Cr3Mo3SiV ≤229
4Cr5MoWVSi ≤235
3Cr3Mo3W2V ≤255
4Cr5Mo2V ≤220
3Cr3Mo3V ≤229
4Cr5Mo3V ≤229
3Cr3Mo3VCo3 ≤229
00Ni18Co8Mo5TiAl  
Ni53Cr19Mo3TiNb ≤300

 

Available Shapes from Fushun

*Round Bar

*Flat Bar

*Block

*Plate

 

Contact Information

[email protected]

Welcome your inquiry. We will send you a free quotation within 24 hours.

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x