manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

Injection Mould Tool Steel

Injection Mould Tool Steel

Injection Mould Tool Steel

Fushun are main manufacturer of tool steel for Injection Mould.

 

What is Injection Mould?

An injection mold is a specialized tool used in the manufacturing process of plastic products through injection molding. It consists of two main parts: the core (male) and cavity (female), which when closed together form the shape of the desired plastic product. These precision-engineered molds are essential components in mass production, enabling manufacturers to produce complex plastic parts with high accuracy and consistency.

The primary function of injection molds is to receive molten plastic material injected under high pressure and temperature, shape it according to the mold design, and cool it to form the final product. These molds also incorporate various features such as cooling channels, ejector systems, runners, gates, and vents to ensure proper material flow, cooling, and part ejection. They are designed to withstand thousands of production cycles while maintaining dimensional accuracy and surface quality.

Injection molds are typically manufactured from tool steels and alloys that possess specific characteristics crucial for their performance. These materials exhibit high wear resistance, excellent thermal conductivity, good machinability, and superior hardness. The mold materials must also demonstrate strong resistance to thermal fatigue, corrosion, and mechanical stress. Additional surface treatments and coatings are often applied to enhance durability and improve release properties, ensuring longer mold life and better part quality.

 

Injection Mould Materials

— — 1.2825 95MnWCr5 MnCrWV
— — 1.2824 70MnMoCr8 7CrMn2Mo
H11 SKD6 1.2343 X37CrMoV5-1 4Cr5MoSiV
H13 SKD61 1.2344 X40CrMoV5-1 4Cr5MoSiV1
— — 1.1191 C45U SM45
— —   — SM50
—     — SM55
P20 — 1.2311 35CrMo7 3Cr2Mo

 

Chemical Composition of Injection Mould

Grade C Si Mn Cr W Mo V
MnCrWV 0.90~1.05 0.10~0.40 1.05~1.35 0.50~0.70 0.50~0.70   0.05~0.15
7CrMn2Mo 0.65~0.75 0.10~0.50 1.80~2.50 0.90~1.20   0.90~1.40  
4Cr5MoSiV 0.33~0.43 0.80~1.20 0.20~0.50 4.75~5.50 一 1.10~1.60 0.30~0.60
4Cr5MoSiV1 0.32~0.45 0.80~1.20 0.20~0.50 4.75~5.50   1.10~1.75 0.80~1.20
SM45 0.42~0.48 0.17~0.37 0.50~0.80        
SM50 0.47~0.53 0.17~0.37 0.50~0.80        
SM55 0.52~0.58 0.17~0.37 0.50~0.80 —      
3Cr2Mo 0.28~0..40 0.20~0.80 0.60~1.00 1.40~2.00   0.30~0.55  

 

Properties of Injection Mould Steel

Grade Annealed HBW
MnCrWV ≤255
7CrMn2Mo ≤235
4Cr5MoSiV ≤229
4Cr5MoSiV1 ≤229
SM45 155~215
SM50 165~225
SM55 170~230
3Cr2Mo 235

 

Available Shapes from Fushun

*Round Bar

*Flat Bar

*Block

*Plate

 

Contact Information

[email protected]

Welcome your inquiry. We will send you a free quotation within 24 hours.

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x