What is Mirror-finish Plastic Mould?

A mirror-finish plastic mold is a highly specialized tooling designed to produce plastic parts with an extremely smooth, reflective surface quality that resembles a mirror. These precision molds require exceptional surface finishing techniques, typically achieving surface roughness levels measured in nanometers. The mold construction demands meticulous attention to detail in both design and manufacturing, incorporating advanced polishing techniques and specific surface treatments to achieve and maintain the mirror-like finish required for high-end aesthetic products.

The primary purpose of mirror-finish molds is to produce plastic parts with perfect reflective surfaces without any visible defects such as flow lines, sink marks, or surface imperfections. These molds feature sophisticated temperature control systems to maintain consistent surface quality throughout the production cycle. The design must account for proper venting, optimized material flow patterns, and precise pressure distribution to prevent any surface defects that could compromise the mirror finish. Special attention is given to gate locations and cooling channel layouts to ensure uniform filling and cooling, preventing any surface irregularities.

The materials used in mirror-finish molds must possess specific characteristics to achieve and maintain the ultra-smooth surface finish. These molds require materials with exceptional hardness to resist wear and maintain the mirror finish over extended production runs, superior thermal conductivity for uniform cooling, and excellent polishability to achieve the required surface finish. The mold materials often undergo special heat treatments and surface enhancement processes to improve their wear resistance and surface stability. Additional surface treatments or coatings may be applied to enhance release properties and prevent any surface degradation that could affect the mirror finish of the molded parts. The mold design must also incorporate features to protect the highly polished surfaces during operation and maintenance.

 

Mirror-finish Plastic Mould Materials

— — 1.2825 95MnWCr5 MnCrWV
— — 1.2824 70MnMoCr8 7CrMn2Mo
H11 SKD6 1.2343 X37CrMoV5-1 4Cr5MoSiV
H13 SKD61 1.2344 X40CrMoV5-1 4Cr5MoSiV1
— — 1.1191 C45U SM45
— —   — SM50
—     — SM55
P20 — 1.2311 35CrMo7 3Cr2Mo
— —   40CrMnNiMo8-6-4 3Cr2MnNiMo
— —   — 4Cr2Mn1MoS
— —   — 8Cr2MnWMoVS
— —   — 5CrNiMnMoVSCa
— —   —— 2CrNiMoMnV
— —   — 2CrNi3MoAl
— —   — 1Ni3MnCuMoAl
— —     2Cr13
— —     4Cr13
— —   — 4Cr13NiVSi
—       2Cr17Ni2
  —   X38CrMo16 3Cr17Mo

 

Chemical Composition of Mirror-finish Plastic Mould

Grade C Si Mn Cr W Mo Ni V
MnCrWV 0.90~1.05 0.10~0.40 1.05~1.35 0.50~0.70 0.50~0.70     0.05~0.15
7CrMn2Mo 0.65~0.75 0.10~0.50 1.80~2.50 0.90~1.20   0.90~1.40    
4Cr5MoSiV 0.33~0.43 0.80~1.20 0.20~0.50 4.75~5.50 一 1.10~1.60    0.30~0.60
4Cr5MoSiV1 0.32~0.45 0.80~1.20 0.20~0.50 4.75~5.50   1.10~1.75   0.80~1.20
SM45 0.42~0.48 0.17~0.37 0.50~0.80          
SM50 0.47~0.53 0.17~0.37 0.50~0.80          
SM55 0.52~0.58 0.17~0.37 0.50~0.80 —        
3Cr2Mo 0.28~0..40 0.20~0.80 0.60~1.00 1.40~2.00   0.30~0.55 一  
3Cr2MnNiMo 0.32~0.40 0.20~0.40 1.10~1.50 1.70~2.00   0.25~0.40 0.85~1.15  
4Cr2Mn1MoS 0.35~0.45 0.30~0.50 1.40~1.60 1.80~2.00   0.15~0.25    
8Cr2MnWMoVS 0.75~0.85 ≤0.40 1.30~1.70 2.30~2.60 0.70~1.10 0.50~0.80   0.10~0.25
5CrNiMnMoVSCa 0.50~0.60 ≤0.45 0.80~1.20 0.80~1.20 — 0.30~0.60 0.80~1.20 0.15~0.30
2CrNiMoMnV 0.24~0.30 ≤0.30 1.40~1.60 1.25~1.45   0.45~0.60 0.80~1.20 0.10~020
2CrNi3MoAl 0.20~0.30 0.20~0.50 0.50~0.80 1.20~1.80   0.20~0.40 3.00~4.00  
1Ni3MnCuMoAl 0.10~0.20 ≤0.45 1.40~2.00     0.20~0.50 2.90~3.40  
2Cr13 0.16~0.25 ≤1.00 ≤1.00 12.00~14.00     ≤0.60  
4Cr13 0.35~0.45 ≤0.60 ≤0.80 12.00~14.00     ≤0.60  
4Cr13NiVSi 0.35~0.45 0.90~1.20 0.40~0.70 13.00~14.00     0.15~0.30 0.25~0.35
2Cr17Ni2 0.12~0.22 ≤1.00 150 15.00~17.00   — 1.50~2.50  
3Cr17Mo 0.33~0.45 ≤1.00 ≤1.50 15.50~17.50   0.80~1.30 ≤1.00  

 

Properties of Mirror-finish Plastic Mould Steel

Grade Annealed HBW
MnCrWV ≤255
7CrMn2Mo ≤235
4Cr5MoSiV ≤229
4Cr5MoSiV1 ≤229
SM45 155~215
SM50 165~225
SM55 170~230
3Cr2Mo 235
3Cr2MnNiMo 235
4Cr2Mn1MoS 235
8Cr2MnWMoVS 235
5CrNiMnMoVSCa 255
2CrNiMoMnV 235
2CrNi3MoAl  
1Ni3MnCuMoAl  
2Cr13 220
4Cr13 235
4Cr13NiVSi 235
2Cr17Ni2 285
3Cr17Mo 285

 

Available Shapes from Fushun

*Round Bar

*Flat Bar

*Block

*Plate

 

Contact Information

[email protected]

Welcome your inquiry. We will send you a free quotation within 24 hours.

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]