1. Specifications & Capability

FUSHUN METAL forges gearbox shafts in 18CrNiMo7-6 (1.6587) and 42CrMo4, 300-800 mm in diameter and up to 12 m long. 18CrNiMo7-6 is a carburizing case-hardening steel combining a tough core with a hard, wear-resistant case; 42CrMo4 is a quenched and tempered (QT) grade for general transmission shafts.

The forging ratio is at least 4:1, keeping a controlled grain flow along the shaft axis for maximum bending and torsion fatigue resistance.

Grade / Condition (mm) Rm (MPa) Rp0.2 (MPa) A (%) Surface
18CrNiMo7-6, carburized core 1050-1300 800 min 8 58-62 HRC
42CrMo4, QT up to 250 750-950 520 min 14 –
300-800 – – – Per spec

Values follow EN 10084 for the carburizing grade and EN 10250-3 for the QT grade; case depth, core hardness and surface hardness are agreed to the gearbox design specification.

2. Components & Service Conditions

FUSHUN METAL forges the full set of gearbox transmission parts: input and output shafts, planet carriers and sun shafts for epicyclic stages. These components carry high torque and cyclic bending loads inside wind and industrial gearboxes.

Gear tooth flanks demand a hard, wear-resistant surface, while the shaft core must absorb bending and torsional stress without fracture. The carburizing grade 18CrNiMo7-6 satisfies both through a case-hardened surface over a tough core; the QT grade 42CrMo4 is used where uniform through-section strength is sufficient. The higher nickel in 18CrNiMo7-6 gives deep hardenability and a tough core for the case depths typical of gearbox shafts.

3. Grade Equivalents – 18CrNiMo7-6 / 42CrMo4

Designation Standard Notes
18CrNiMo7-6 / 1.6587 EN 10084 Carburizing case-hardening steel
42CrMo4 / 1.7225 EN 10250-3 QT transmission shaft steel
AISI 9310 SAE J404 US carburizing equivalent
SNCM815 JIS G4053 Japanese equivalent
20Cr2Ni4A GB/T 3077 Reference only, not used in certification
18CrNiMo7-6 gearbox shaft forging
18CrNiMo7-6 gearbox shaft forging
Grade C Si Mn Cr Ni Mo
18CrNiMo7-6 (1.6587) 0.15-0.21 0.40 max 0.50-0.90 1.50-1.80 1.40-1.70 0.25-0.35
42CrMo4 (1.7225) 0.38-0.45 0.40 max 0.60-0.90 0.90-1.20 – 0.15-0.30

The 1.4-1.7% nickel content of 18CrNiMo7-6 provides the deep hardenability required for carburized case depths on gear flanks.

4. Manufacturing Process

Steelmaking. FUSHUN METAL melts in an electric arc furnace with ladle refining and vacuum degassing to keep inclusions low, which is critical for the fatigue resistance of gear teeth.

Forging. The shaft is forged on a 20/80 MN fast forging press with a minimum 4:1 reduction ratio, orienting grain flow along the load path.

Heat treatment. 18CrNiMo7-6 parts are carburized and hardened to the specified case depth and surface hardness; 42CrMo4 parts are quenched and tempered.

Testing. Full-section UT, hardness and case-depth verification, with complete heat traceability for every shaft.

5. Standards & Certification

Gearbox shafts are supplied to EN 10084 (case-hardening steel) and EN 10250-3 (QT steel forgings), with inspection certificates under EN 10204 3.1. FUSHUN METAL holds ISO 9001 and AS9120B certification with complete heat traceability for every shaft.

Related forging: wind turbine main shafts.

6. Typical Applications

Wind gearboxes

Input and output shafts for wind turbine gearboxes.

Planet carriers

Forged planet carriers with integral pinion journals.

Sun shafts

Central sun gear shafts for epicyclic stages.

Industrial gearboxes

Transmission shafts for industrial gearing packages.

7. Inquiry Essentials

To quote your gearbox shaft, please provide the gear shaft drawing, the required carburizing depth or hardness range, the core and surface hardness requirements, and the applicable standard.

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x