manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

RPV Forgings

1. Specifications & Capability

FUSHUN METAL forges reactor pressure vessel (RPV) components in SA-508 Gr.2/3, 16MND5, 18MND5 and 20MnMoNi5-5, from vacuum-cast ingots up to 114 t and single pieces up to the 100 t class. Final dimensions are established through project-specific process qualification.

These forgings cover the full primary pressure boundary, produced to ASME and RCC-M with third-party surveillance and EN 10204 3.2 certification.

Grade Standard Typical Use
SA-508 Gr.3 ASME SA-508 RPV shell, head, nozzles
16MND5 RCC-M Steam generator heads, tubesheets
20MnMoNi5-5 / 1.6310 EN 10222 European RPV steel

2. Components & Service Conditions

FUSHUN METAL forges the complete RPV set: shell courses, transition rings, nozzle shells, the closure head, the bottom head, nozzles, pressuriser shell courses, steam generator heads and tubesheets, and main coolant pump casings. These components form the primary pressure boundary, containing the reactor coolant at operating pressure and temperature.

Near the core the steel sees neutron irradiation, so copper and vanadium are tightly controlled to resist irradiation embrittlement. Multiple-ladle casting with inverse-segregation compensation and vacuum treatment secures the internal soundness of the 100 t class sections, and full-section ultrasonic testing plus third-party surveillance confirm compliance with the nuclear code.

3. Grade Equivalents – SA-508 Gr.3 / 16MND5

Designation Standard Notes
SA-508 Gr.2/3 ASME SA-508 US RPV steels
16MND5 / 18MND5 RCC-M French RPV steels
20MnMoNi5-5 / 1.6310 EN 10222 European RPV steel
20MnMo JB/T Reference only, not used in certification
SA-508 reactor pressure vessel forging
SA-508 reactor pressure vessel forging
Grade C Si Mn Cr Mo Ni
SA-508 Gr.3 0.25 max 0.15-0.40 1.20-1.50 0.25 max 0.45-0.60 0.40-1.00
16MND5 0.20 max 0.10-0.30 1.15-1.55 0.25 max 0.45-0.55 0.50-0.80

Copper and vanadium are controlled to resist neutron irradiation embrittlement over the vessel’s 40-60 year design life.

4. Manufacturing Process

Melting & casting. FUSHUN METAL uses multiple-ladle pouring with inverse-segregation compensation and vacuum casting up to 114 t, controlling copper, vanadium and residual elements for irradiation resistance.

Forging. Shell courses, heads and nozzle shells are forged as single pieces with a high reduction ratio, compacting the core and closing central porosity.

Heat treatment. Quenching and tempering set the strength and toughness required for the primary boundary.

Testing. Full-section UT, mechanical and impact tests, and third-party surveillance with EN 10204 3.2 certification and complete traceability.

5. Standards & Certification

RPV forgings are supplied to ASME SA-508 and RCC-M, with EN 10204 3.2 certificates and third-party surveillance. FUSHUN METAL holds ISO 9001 and AS9120B certification.

Related forgings: nuclear flange rings and heat exchanger tubesheets.

6. Typical Applications

Pressurised water reactors

RPV shells, heads and nozzles for PWR plants.

Steam generators

Heads and tubesheets for nuclear steam generators.

Pressurisers

Pressuriser shell courses for primary circuit control.

Coolant pumps

Main coolant pump casings for the primary loop.

7. Inquiry Essentials

To quote your RPV forging, please provide the component drawing, the reactor type, the required grade, and the third-party surveillance requirements.

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x