manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

Large Forged Flanges

1. Specifications & Capability

FUSHUN METAL forges large flanges – weld neck, blind and ring type – in F11, F22, F91, F304, F316 and F51, DN300-1500 mm, for petrochemical and power plant piping. Flanges are integrally forged, machined, and tested by ultrasonic and magnetic particle inspection.

Forging the flange from a single piece, with grain flow following the hub-to-ring contour, gives the pressure integrity a manway or nozzle connection demands, without the weld seam of a fabricated flange.

Grade Standard Type
F11 / F22 / F91 ASTM A182 Cr-Mo alloy steel
F304 / F316 ASTM A182 Austenitic stainless
F51 ASTM A182 Duplex stainless

2. Components & Service Conditions

These flanges are the manway and nozzle flanges of pressure vessels and the connection flanges of power plant piping. They seal against a gasket under pressure while carrying the bolting load, so both strength and the integrity of the sealing face matter.

The Cr-Mo grades (F11, F22, F91) are selected for elevated-temperature strength and hydrogen service, the austenitic F304/F316 for corrosion resistance, and the duplex F51 where chloride stress-corrosion cracking is a risk. The flange is integrally forged so the grain flow follows the hub contour, and ultrasonic plus magnetic particle inspection confirm soundness at the sealing surface.

3. Grade Equivalents – F11 / F22 / F91 / F304 / F316

Designation Standard Notes
F11 ASTM A182 1.25Cr-0.5Mo
F22 ASTM A182 2.25Cr-1Mo
F91 ASTM A182 9Cr-1Mo-V
F304 / F316 ASTM A182 Austenitic stainless
F51 ASTM A182 Duplex stainless
13CrMo4-5 / 10CrMo9-10 EN 10222 European equivalents
F22 large forged flange
F22 large forged flange
Grade C Mn Cr Ni Mo
F22 0.05-0.15 0.30-0.60 2.00-2.50 – 0.87-1.13
F304 0.08 max 2.0 max 18.0-20.0 8.0-11.0 –
F316 0.08 max 2.0 max 16.0-18.0 10.0-14.0 2.00-3.00

The chromium-molybdenum grades give elevated-temperature strength and hydrogen resistance; F316’s molybdenum improves pitting resistance over F304.

4. Manufacturing Process

Forging. FUSHUN METAL integrally forges the flange from a single billet, with grain flow following the hub-to-ring contour.

Heat treatment. Cr-Mo grades are quenched and tempered; stainless grades are solution annealed.

Machining. The flange is machined to the standard or drawing, including the gasket face and bolting holes.

Testing. UT and MT, with full traceability and inspection certificates under EN 10204 3.1.

5. Standards & Certification

Large forged flanges are supplied to ASTM A182 and EN 10222, with inspection certificates under EN 10204 3.1. FUSHUN METAL holds ISO 9001 and AS9120B certification.

Related forgings: wind turbine flanges and nuclear flange rings.

6. Typical Applications

Manway flanges

Flanges for pressure vessel manways.

Nozzle flanges

Flanges for vessel and pipe nozzles.

Power plant piping

Connection flanges for power station piping.

Petrochemical

Flanges for petrochemical process piping.

7. Inquiry Essentials

To quote your forged flange, please provide the flange standard, pressure rating, facing type, and the required grade.

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x