6 Key Heat Treatment Questions to Deepen Your Understanding

6 Key Heat Treatment Questions to Deepen Your Understanding 1. What Is Annealing of Steel? What Are Its Types and Applications? Annealing is a heat treatment process in which steel is heated to a temperature above or below its critical point (AC1), held for a specific time,

Read more →

Why Do Metals Suddenly “Break”?

Why Do Metals Suddenly “Break”? A Technical Expert’s Perspective on Metal Brittleness In our daily lives and engineering projects, metals are everywhere: from bridges and high-speed rails to aircraft and automobiles, metals serve as critical materials. But did you know? These seemingly robust metals can sometimes become

Read more →

Development History of Super Austenitic Stainless Steel

  Development History of Super Austenitic Stainless Steel Super austenitic stainless steel is a type of austenitic stainless steel with high Cr, Mo, N content and a pitting resistance equivalent number (PREN) of no less than 40. Compared with conventional austenitic stainless steel, super austenitic stainless steel

Read more →

FUSHUN METAL Expands Market Insights at the 2025 Korea Die & Mold Show

FUSHUN METAL Expands Market Insights at the 2025 Korea Die & Mold Show Published: March 15, 2025 | Author: FUSHUN METAL Marketing Department | Reading Time: 5 minutes In a strategic move to enhance its industry knowledge and strengthen international partnerships, a delegation from FUSHUN METAL recently

Read more →

Improving Comprehensive Yield Rate of H13 Die Steel Forging: A Technical Analysis

Improving Comprehensive Yield Rate of H13 Die Steel Forging: A Technical Analysis In the field of hot work die steel manufacturing, FUSHUN METAL has conducted extensive research on improving the comprehensive yield rate of H13 die steel forgings. This analysis explores the key factors affecting yield rates

Read more →

Chinese New Year Holiday Notice 2025

Dear Valued Customers, We would like to inform you that Fushun Metal will be closed for the Chinese New Year holiday from January 24th to February 5th, 2025. We will resume normal operations on February 6th, 2025. During this period, our email address [email protected] will remain monitored

Read more →

Research on the Process to Improve the Uniformity of Eutectic Carbides in Tool Steel

Cr12MoV tool steel is a typical cold-work tool steel, accounting for 17% of the total tool steel production and 34% of alloy tool steel production. It has excellent hardenability, quenching and tempering hardness, wear resistance, and strength. It is used to manufacture various cold punching dies and

Read more →

Tempering Microstructure and Hardness of P20 Plastic Mold Steel

Introduction P20 plastic mold steel is a widely utilized material due to its simple metallurgical production process, high yield rate, and affordability. It exhibits good machinability within the pre-hardened hardness range of 28–35 HRC, excellent hardenability for achieving uniform hardness in large cross-sections, and superior mirror polishing

Read more →

Empowering Our Team for a Stronger Future – 2024 Strategic Training in Shenzhen

At Fushun Special Steel, we believe that our employees are the foundation of our success. As part of our commitment to growth and development, we are proud to announce a high-impact training program for our Finance, Sales, and Procurement Department Managers, scheduled to take place in mid-December

Read more →

Ultrasonic Testing Based Method for Detecting Internal Defects in H13 Tool Steel

H13 tool steel, known for its excellent thermal stability, wear resistance, and high toughness, is widely used in hot working molds. However, during the casting and processing of mold steel, internal defects can occur, which become a critical factor limiting the performance and service life of mold

Read more →

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x