manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

DIN EN10308 2002 Non-destructive Testing Ultrasonic Testing of Steel Bars

EN 10308 defines ultrasonic testing of steel bars — how the test is performed and, more importantly, how acceptance is classified. It is the standard behind a purchase order that says “UT to EN 10308” without saying which class, which is a specification that cannot be quoted against.

What the standard fixes

  • Test classes — typically three, from detection of larger defects only to the most sensitive
  • Reference reflector sizes and how they are used for calibration
  • Scanning coverage, including whether the whole cross-section or the periphery is examined
  • Acceptance criteria: what counts as a defect and what is permitted
  • Documentation and personnel qualification

The class decides the price. Moving from the loosest to the tightest class can double the testing time, because it changes both the sensitivity and how much of the bar is scanned.

Why “UT” alone is not a requirement

Two suppliers quoting “UT to EN 10308” can be quoting entirely different tests. One may scan the surface zone and accept a 3 mm defect; the other may scan the full section and reject it. Both are compliant with the words on the order.

What to put on the order

  • The test class, by number
  • Reference size and acceptance level
  • Whether the whole cross-section or the periphery is examined
  • Test after machining or on the black bar
  • Whether a third-party inspector has to witness

For bar that will be drilled or bored, the test has to reach the centre. For bar that will be turned, the near-surface zone matters more — and the class should reflect which.

Download the standard

EN 10308 — Non-destructive testing, ultrasonic testing of steel bars (PDF)

Related reading

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x