manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

Heavy Press Crossbeam Forgings

1. Specifications & Capability

FUSHUN METAL produces heavy crossbeams for hydraulic presses – the upper, middle and lower beams – in single pieces of 50-333 t, with a production record of a 333 t beam. Construction is forged, welded, or a forged-and-welded combination, machined to close tolerances.

These are the largest structural forgings FUSHUN METAL supplies, produced to EN 10025 and the user specification with full traceability.

Grade Standard Single Weight
Forged steel (S355 / 42CrMo4) EN 10025 / EN 10250-3 50-333 t
Cast steel User specification Up to 400 t

2. Components & Service Conditions

The crossbeams are the structural members of the press frame: the upper beam carries the main cylinder, the lower beam supports the work, and the moving beam transmits the pressing force. They carry the full pressing load in bending, so both strength and stiffness govern the design.

For the largest beams a forged-and-welded construction combines forged sections of verified soundness with welded assembly, giving a strong, stiff frame without the internal defects that would limit a pure casting. Each beam is machined to close tolerances so the press guides and cylinder seats align precisely under load.

3. Grade Equivalents – S355 / 42CrMo4

Designation Standard Notes
S355J2+N / 1.0577 EN 10025 Structural steel
42CrMo4 / 1.7225 EN 10250-3 QT alloy steel
Cast steel User specification Cast option up to 400 t
Q345 GB/T 1591 Reference only, not used in certification
Heavy press crossbeam forging
Heavy press crossbeam forging
Grade C Si Mn Cr Mo
S355J2+N (1.0577) 0.20 max 0.55 max 1.60 max – –
42CrMo4 (1.7225) 0.38-0.45 0.40 max 0.60-0.90 0.90-1.20 0.15-0.30

S355 is the standard frame steel; 42CrMo4 is used where higher strength or wear resistance at the guides is required.

4. Manufacturing Process

Forging & welding. FUSHUN METAL forges the beam sections on an 80 MN press, then assembles them by welding into the finished frame member where a forged-and-welded construction is specified.

Heat treatment. Stress relief and normalising are applied to the welded assembly to stabilise dimensions.

Machining. The beam is machined to close tolerances on guide ways, cylinder seats and locating faces.

Testing. UT, weld inspection and dimensional verification, with full traceability.

5. Standards & Certification

Crossbeams are supplied to EN 10025 and the user specification, with inspection certificates under EN 10204 3.1. FUSHUN METAL holds ISO 9001 and AS9120B certification.

Related forgings: press columns and press cylinders.

6. Typical Applications

Upper beams

Upper crossbeams carrying the main cylinder.

Middle beams

Moving crossbeams for the press ram.

Lower beams

Lower crossbeams supporting the work.

Forging presses

Frame members for large hydraulic forging presses.

7. Inquiry Essentials

To quote your crossbeam, please provide the beam drawing, the tonnage, and the machining tolerance requirements.

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x