High Precision Steel Bar Used in CNC Machine

High Precision Steel Bar Used in CNC Machine

High Precision Steel Bar Used in CNC Machine

We focus on the development and production of centering machine materials. We serve the users of centering machine and automatic lathe machining. We are dedicated to the development and production of automatic feeding high precision metal bars. 96% of our customers are centering machine machining companies.

 

Advantage

Tolerance: 0.02mm

Straightness: 0.05mm/M

Ovality: 0.10mm

 

Dimensions

Diameter: 1 to 50mm

Width: 1 to 40mm

Available shapes

  • Round
  • Hexagonal
  • Square
  • Regular shaped cross section
  • Special shapes (on request)

 

Materials

  • Carbon steel
  • Alloy Steel
  • Stainless steel

*follow standard EN/DIN/ASTM/JIS

 

Package

Wrapped by plastic sheet, nylon sheet. Then put into wooden case.

Application

  • CNC machine tools
  • slitter machine tools
  • turning-milling complex machine tools
  • automatic lathes
  • computer lathes
  • CNC Pump
  • valve hydraulic systems
  • electromagnetic parts
  • automotive parts
  • precision pivots
  • Medical instruments
  • spool stem
  • Marine parts.

 

What “high precision” has to mean

A bar sold as high-precision for CNC work is not defined by its grade. It is defined by four things: diameter tolerance, straightness, surface condition and residual stress. A bar that meets the first two but carries residual stress will still move when the first cut removes material from one side.

That is why the specification has to cover all four, and why two suppliers can both quote “high precision bar” and deliver very different machining behaviour.

The four requirements

Property Why it matters on a CNC
Diameter tolerance Collet grip, bar feeder clearance, and how much the first pass has to remove
Straightness Bar feeder jams, vibration, and taper on long parts
Surface Tool life and the finish on any as-turned surface
Residual stress The part bends after machining — the most expensive of the four

What to put on the order

Tolerance class (h9 or better), straightness over a stated length, whether the bar is cold drawn or ground, and whether it is stress relieved. If the part is long and slender, add the stress relief explicitly — it is the difference between a part that stays straight and one that has to be straightened after machining, which no one wants to do.

Related reading

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x