manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

Pressure Shell Forgings

1. Specifications & Capability

FUSHUN METAL forges high-pressure gas cylinders and pressure hull sections in AISI 4340 ultra-clean steel, vacuum-degassed for maximum cleanliness, to custom sizes for deep-sea and defence applications. Components are forged as single pieces, quenched and tempered, and full-section ultrasonically tested.

Forging a pressure shell from one piece removes the weld seams that are the weak points under cyclic pressure, giving the integrity a deep-sea hull or high-pressure cylinder demands.

Grade Standard Typical Use
AISI 4340 AMS / MIL Pressure hull, gas cylinders
1.6957 / 26NiCrMoV14-5 EN 10250-3 European equivalent

2. Components & Service Conditions

These forgings are the pressure hull sections of submersibles and the bodies of high-pressure gas cylinders, holding internal pressure against external water depth or containing gas at several hundred bar. Both are fatigue-critical pressure boundaries.

The ultra-clean, vacuum-degassed 4340 gives the strength and toughness for these thick sections, while forging from a single piece eliminates the weld seams that limit fatigue life. Quenching and tempering sets the ordered strength, and full-section ultrasonic testing confirms freedom from the internal defects that could fail under cyclic pressure at depth.

3. Grade Equivalents – AISI 4340

Designation Standard Notes
AISI 4340 SAE J404 / AMS Ni-Cr-Mo high-strength steel
26NiCrMoV14-5 / 1.6957 EN 10250-3 European equivalent
30Cr2Ni4MoV GB/T 8732 Reference only, not used in certification
AISI 4340 pressure shell forging
AISI 4340 pressure shell forging
Grade C Si Mn Cr Ni Mo
AISI 4340 0.38-0.43 0.15-0.35 0.60-0.80 0.70-0.90 1.65-2.00 0.20-0.30

The 1.65-2.00% nickel gives the deep hardenability and toughness needed for thick pressure sections; the vacuum degassing keeps inclusions low for fatigue life.

4. Manufacturing Process

Melting. FUSHUN METAL produces ultra-clean steel with vacuum degassing, keeping inclusions low for maximum fatigue life.

Forging. The shell is forged as a single piece, eliminating weld seams and aligning grain flow with the pressure boundary.

Heat treatment. Quenching and tempering set the ordered strength and toughness.

Testing. Full-section UT, mechanical tests, and pressure verification, with full traceability.

5. Standards & Certification

Pressure shells are supplied to AMS and military specifications, with inspection certificates under EN 10204 3.1. FUSHUN METAL holds ISO 9001 and AS9120B certification.

Related forging: gun barrels.

6. Typical Applications

High-pressure cylinders

Bodies for high-pressure gas cylinders.

Pressure hull sections

Hull sections for submersibles and deep-sea craft.

Defence

Pressure forgings for defence applications.

Deep-sea equipment

Pressure vessels for deep-sea equipment.

7. Inquiry Essentials

To quote your pressure shell, please provide the shell drawing, the design depth or pressure, and the material specification.

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x