15CDV6, 1.7734, Alloy Steel
What Is 15CDV6?
15CDV6 / 1.7734 is chromium-molybdenum-vanadium structural alloy steel. It is a heat-resistant CrMoV-alloyed tempering steel with high strength, which is often used for components with high loads in motorsport, industry and aviation. Among others, 15CDV6 is used for the manufacture of rocket engines, parts for electric motors, extremely light and durable aircraft components and structures, vehicle frames in motorsport or important components in the nuclear and defense industries.
The material has excellent weldability, toughness and good bending capabilities.
15CDV6 can be welded with no risk of cracking or weak welds and doesn’t require any pre or post-weld heat treatment when fabricated in the fully heat treated condition. This makes complicated engineering and manufacture of the material easier to work with.
Due to its excellent mechanical properties, the material 1.7734 / 15CDV6 has found its way to the top end of Motorsport, Aerospace and the Defence sectors. Used in all forms for the highest of demands.
Chemical Composition of 1.7734 / 15CDV6
| C: | 0,12 – 0,18 % |
| Mn: | 0,8 – 1,1 % |
| Si: | max. 0,2 % |
| P: | max. 0,02 % |
| S: | max. 0,015 % |
| Cr: | 1,25 – 1,5 % |
| Mo: | 0,8 – 1,0 % |
| V: | 0,2 – 0,3 % |
Specifications
LN9369 / AIR9160C / ASNA3108 / ASNA6078 / EN2218 / EN2219 / EN2251
1.7734 Mechanical Properties
| Alloy | Condition | Tensile Strength MPa | Yield Strength MPa | Elongation % | Hardness HB |
| Alloy 15CDV6 | 1.7734.2 (ann) | – | – | – | 197 |
| Alloy 15CDV6 | 1.7734.4 | 700 | 550 | 13 | 207 |
| Alloy 15CDV6 | 1.7734.5 | 980-1180 | 790 | 11 | 293-352 |
| Alloy 15CDV6 | 1.7734.6 | 1080-1250 | 930 | 10 | 321-363 |
Equivalent grades — and why there is no AISI twin
15CDV6 is a European aerospace grade and is not issued under an AISI/SAE number. Buyers searching for “15CDV6 equivalent” usually want to know whether an American grade can be substituted: for most aerospace applications it cannot, because the qualification is tied to the European specification and its test schedule, not just to the chemistry.
| System | Designation |
|---|---|
| DIN / EN (W.-Nr.) | 1.7734 |
| AFNOR | 15CDV6 |
| AISI / SAE | No direct equivalent — nearest chemistry is a low-carbon CrMoV steel, but no AISI grade matches the specification |
| Typical supply standard | European aerospace material specifications, normally on a qualified-mill basis |
The nearest American grades in composition are 4130 and 4140, but neither carries the vanadium addition or the aerospace qualification. Treat them as a reference point, not as a substitute.
Related reading
- 25CrMo4 / 1.7218 — the plain CrMo steel this grade is alloyed up from.
- AISI 4130 — closest American chemistry for tube and airframe work.
- Aerospace steel solutions — the AMS-certified grades and melting routes we supply.
- What is quenching — how the cooling rate behind the strength figures is controlled.
You get chemical composition, mechanical properties and a price — with inspection certificates to EN 10204 3.1 issued against the heat number.