manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

DIN 1.6587 X4317 18CrNiMo7-6 17CrNiMo6 18NCD6 Case Hardening Steel Bar

DIN 1.6587 X4317 18CrNiMo7-6 17CrNiMo6 18NCD6 Case Hardening Steel Bar

DIN 1.6587 X4317 18CrNiMo7-6 17CrNiMo6 18NCD6 Case Hardening Steel Bar

DIN1.6587 X4317 18CrNiMo7-6 17CrNiMo6 18NCD6 Case Hardening Steel Bar

1. 1.6587 Application

EN 1.6587 steel is an alloy steel formulated for primary forming into wrought products. 1.6587 is the EN numeric designation for this material. … It has a moderately high density among EN wrought alloy steels. In addition, it has a fairly high base cost and a moderately high electrical conductivity. Severely stressed components for mechanical engineering and automobile industry, gear for mining, cement plants, power plants, mobile cranes and earth-moving equipment, paper mill, sugar mill, marine, wind gear, railway systems, oil platform, etc.

2.All Grades Comparison

DIN EN ANFOR AS
1.6587 18CrNiMo7-6 18NCD6 X4317

3.Quality Standard

EN 10084 Case hardening steels
DIN17210 Case hardening steels
AS1444 Wrought alloy steels

4.Chemical Composition(%)

C Mn Si P S Cr Ni Mo
0.15-0.21 0.50-0.90 0.40 max 0.025 max 0.025 max 1.50-1.80 1.40-1.70 0.25-0.35

5.Mechanical Properties(T=20°C if not differently stated)

Process Diameter(mm) Tensile Strength Rm (Mpa) Yield Strength Rp0.2 (Mpa) Elongation A5 (%) Area Reduction Ratio C (%) Impact Value Kv (J) Room Temperature Hardness (HB)
SOFT ANNEALED / / / / / / 229 max
NORMALIZED / / / / / / 140-210
QUENCHED AND TEMPERED 11 max 1180-1420 835 min 7 min 30 min 44 min 354-406
QUENCHED AND TEMPERED 12-30 1080-1320 785 min 8 min 35 min 44 min 327-384
QUENCHED AND TEMPERED 31-63 980-1270 685 min 8 min 35 min / 295-373
QUENCHED AND TEMPERED 100-160 1000-1200 800 min 11 min 50 min 45 min 295-353
QUENCHED AND TEMPERED 160-250 1000-1200 800 min 11 min 50 min 45 min 295-353

6.HEAT TREATMENT:

  • Soft Annealing: Heat 17CrNiMo6 to 650-700oC, cool slowly in furnace. This will produce a maximum Brinell hardness of 229.
  • Normalizing: 850-880oC, air.
  • Hardening: Carburising: 880-980oC. Core Hardening: 830-870oC, water. Case Hardening: 780-820oC, water.
  • Tempering:Temperature: 150-200oC

7.Forging:

Hot forming temperature: 1100-900oC.

8.Welding:

Pre-heat welding area to 250-450°C and maintain this temperature while welding with a low hydrogen electrode. Cool 17CrNiMo6 at a maximum rate of 100°C per hour. Weld before carburising.

9.Mill′s test certificate:

EN 10204/3.1 with all relevant data reg. chem. composition, mech. properties and results of testing.

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : info@fushunspecialsteel.com

x