manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

SUP7 1.5028 56Si7 9260H 60Si2Mn Spring Steel

SUP7 1.5028 DIN 56Si7 SAE 9260H 60Si2Mn Spring Steel

SUP7 Mat.No. 1.5028 DIN 56Si7 SAE 9260H 60Si2Mn  Spring Steel p1

SUP7 Mat.No. 1.5028 DIN 56Si7 SAE 9260H 60Si2Mn Spring Steel p1

Mat.No. 1.5028 DIN 56Si7 SAE 9260H 60Si2Mn SUP7 Spring Steel Strip


Mat.No. 1.5028 DIN 56Si7 SAE 9260H 60Si2Mn Spring Steel Strip

Mat.No. 1.5028 DIN 56Si7 SAE 9260H 60Si2Mn SUP7 Spring Steel Wire


Mat.No. 1.5028 DIN 56Si7 SAE 9260H 60Si2Mn Spring Steel Wire

1 Sup7 Introduction:

JIS SUP7 Steel is a high quality Alloy Spring Steel, It belong to the high quality high carbon alloy Spring Steel. Quenched & Tempered Hardness is 28-34 HRc. SUP 7 steel Annealing delivery hardenss less than 250HB.

2 SUP7 Applications:

Steel grade for laminated springs thickness above 7 mm for trucks and railway vehicles, coiled and threaded springs.

3 Quality Standard:

JIS G4801 2005 Spring Steels
BS EN 10089 2002 Hot rolled steels for quenched and tempered springs
ASTM A29 Standard Specification Steel Bars, Carbon and Alloy, Hot-Wrought, General Requirements

4 All Grades Comparison:

Material No. EN JIS ASTM GB
1.5028 56Si7 SUP7 9260H 60Si2Mn

5 SUP7 Chemical Composition(%)

Steel Grade C Si Mn P S
9260 0.56-0.64 1.90-2.20 0.75-1.00 0.035 max 0.040 max
56Si7 0.52-0.60 1.60-2.00 0.60-0.90 0.025 max 0.025 max
SUP7 0.56-0.64 1.80-2.20 0.70-1.00 0.030 max 0.030 max
60Si2Mn 0.56-0.64 1.50-2.00 0.70-1.00 0.035 max 0.035 max

6 HEAT TREATMENT:

  • FORGING:Hot forming temperature: 1050-850oC.
  • SOFT ANNEALING: Heat to 640-680oC, cool slowly in furnace. This will produce a maximum Brinell hardness of 255.
  • HARDENING: Harden from a temperature of 830-860oC followed by oil quenching.
  • TEMPERING:Tempering temperature: 350-550oC, air.

7 Mill′s test certificate:

EN 10204/3.1 with all relevant data reg. chem. composition, mech. properties and results of testing.

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : info@fushunspecialsteel.com

x