manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

SCM435 Alloy Steel

SCM435 Alloy Steel

Grade : SCM435

Classification: Structural steel Chromium molybdenum steel

Standards: JIS G 4053 : Low-alloyed steels for machine structural use

 

Our supply size :

Diameter : 80 to 600 mm ;

Length : 1000 to 9000 mm ;

 

Our advantage :

  1. High Quality, Reasonable Price
  2. Over 40 Years Experience
  3. ISO NQA Certificated Factory
  4. Worldwide shipping
  5. Emergency Orders and Fast Delivery

 

Equivalent steel grade

GB ASTM/SAE/AISI DIN SCM
35CrMo 4135 34CrMo4 SCM435

 

Chemical composition % of grade SCM435

C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Mo(%) Cu(%)
0.33-0.38 0.15-0.35 0.60-0.85 ≦0.03 ≦0.03 0.9-1.2 0.15-0.30 ≦0.3

 

scm435 steel is a Chromium-Molybdenum through-hardening steel of medium hardenability. It is a general purpose high-tensile steel with medium strength level and good impact properties.

 

Application

scm435 steel bar is mainly used to produce high strength stud bolt, Threaded Rods , wind power bolt, pre-stressed anchor bolts, post stressed anchor bolt, Steel Tie Rod , tie bar, tension rod, Tension Bar etc. Shaft, axle shaft, crankshaft, shaft for sleeve, linear shaft, pump shaft, rotor shaft, sensor shaft, spline shaft, drive shaft, mandrel shaft, transmission shaft, screw rod etc. CNC machines, precision CNC machines etc. Ejector pins and Ejector rods.

 

Quenched and tempered properties:

Yield strength of scm435 steel: 930MPa min

Tensile strength of scm435 steel: 1080MPa min

Elongation of 34CrMo4 steel: 12% min

Reduction area of scm435 steel: 50% min

Rockwell hardness of scm435 steel: 32HRC min

Brinell hardness of annealed scm435 steel: 217HB max

 

Forming Option

1 Hot rolling process

2 Hot Forging: Electro-hydraulic; High-speed-hydraulic; Oil-hydraulic; Precision-forging

 

Heat-treatment Option

1 +A: Annealed (full/soft/spheroidizing)

2 +N: Normalized

3 +NT: Normalized and tempered

4 +QT: Quenched and tempered (water/oil)

 

Surface Option

1 Black Surface

2 Grounded: Bright but rough ; Not precision

3 Machining for plate: Bright and precision; Little turning scar

4 Peeled/Turned: Bright and precision; Little turning scar

5 Polished: Very Bright and precision size; Not turning scar

 

Other Services

1 Cutting: Small pieces

2 CNC Machine: Produce as your drawing

3 Package: Bare/Nylon/Canvas/Wooden

4 Payment:T/T, L/C, O/A(request credit)

5 Transport:FOB/CFR/CIF/DDU/DDP (train/ship/Air)

 

Mill test certificate

EN 10204/3.1 with all relevant data reg. chem. composition, mech. properties and results of testing.

 

We also supply :

4130 , 4130 p+x , 4140 , 4330v mod , 4340 , 4145h mod , 4317

1.8509 , 1.6523 , 1.7707 , 1.6657 , 1.6587 , 1.6582 , 1.6773

For all products, please check here: Fushun products

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.