SCM440 Alloy Steel Grade SCM440 Classification Structural steel Chromium molybdenum steel StandardsJIS G 4053 Low-alloyed steels for machine structural use Our supply size Diameter 80 to 600 mm ; Length 1000 to 9000 mm ; Our advantage 1. High Quality, Reasonable Price 2. Over 40 Years Experience 3. ISO NQA Certificated Factory 4. Worldwide shipping 5. Emergency Orders and Fast Delivery Comparison of Materials EU INTER USA JAPAN GERMANY CHINA EN ISO AISI JIS DIN GB 42CrMo4 42CrMo4 4140 SCM440 42CrMo4 42CrMo Chemical Composition(JIS G4051) C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Mo(%) Ni(%) Cu(%) 0.38-0.43 0.15-0.35 0.6-0.85 0≦0.03 0≦0.03 0.9-1.2 0.15-0.3 0≦0.25 0≦0.3 Introduce SCM440 is medium carbon chromium molybdenum alloy steel, which is an alloy steel containing chromium and molybdenum. It has the advantages of stable composition, low harmful elements, high steel purity, small decarburization layer and few surface defects. It is easy to be spheroidized and has low cold cracking rate. It is usually hardened and tempered. The ultimate tensile strength is 850-1000 Mpa. This material achieves a very good balance between strength, toughness and wear resistance. The chromium content of the alloy provides good hardness permeability, and the molybdenum element imparts average hardness and high strength. SCM440 reacts well in heat treatment and it is easy to process under heat treatment conditions. This material provides many desirable properties such as good strength and wear resistance, excellent toughness, good ductility and resistance to high-temperature stresses. Product Features 1. High strength and toughness. 2. Great property of quenching and can be deep hardened. 3. Less tempering brittleness tendency. 4. Great machining performance under high temperature and nice appearance after machining. 5. Good performance in weld ability. 6. Excellent performance in impact absorption, such as where the hammer may bounce back and has barely any damage caused upon impact. Conditions of heat treatment Annealing 830℃ Furnace Cooling Normalization 830~880℃ Air Cooling Hardening 830~880℃ Oil Cooling Tempering 530~630℃ Rapid Cooling Criterion for heat treating conditions revise Ac 750~790℃ Ar 740~690℃ Ms 310℃ Mechanical properties Tensile strength (kgfmm²) ≧100 Yield strength (kgfmm²) ≧85 Elongation (%) ≧12 Cross section reduction rate (%) ≧45 Impact value (Jcm2) ≧6 Hardness (Hb) 285~352 Forming Option 1 Hot rolling process 2 Hot Forging Electro-hydraulic; High-speed-hydraulic; Oil-hydraulic; Precision-forging Heat-treatment Option 1 +A Annealed (fullsoftspheroidizing) 2 +N Normalized 3 +NT Normalized and tempered 4 +QT Quenched and tempered (wateroil) Surface Option 1 Black Surface 2 Grounded Bright but rough ; Not precision 3 Machining for plate Bright and precision; Little turning scar 4 PeeledTurned Bright and precision; Little turning scar 5 Polished Very Bright and precision size; Not turning scar Other Services 1 Cutting Small pieces 2 CNC Machine Produce as your drawing 3 Package BareNylonCanvasWooden 4 PaymentTT, LC, OA(request credit) 5 TransportFOBCFRCIFDDUDDP (trainshipAir) Mill test certificate EN 102043.1 with all relevant data reg. chem. composition, mech. properties and results of testing. We also supply 4130 , 4130 p+x , 4140 , 4330v mod , 4340 , 4145h mod , 4317 1.8509 , 1.6523 , 1.7707 , 1.6657 , 1.6587 , 1.6582 , 1.6773 For all products, please check here Fushun products

Grade :SCM440

Classification: Structural steel Chromium molybdenum steel

Standards:JIS G 4053 : Low-alloyed steels for machine structural use

 

Our supply size :

Diameter : 80 to 600 mm ;

Length : 1000 to 9000 mm ;

 

Our advantage :

  1. High Quality, Reasonable Price
  2. Over 40 Years Experience
  3. ISO NQA Certificated Factory
  4. Worldwide shipping
  5. Emergency Orders and Fast Delivery

 

Comparison of Materials

EU INTER USA JAPAN GERMANY CHINA
EN ISO AISI JIS DIN GB
42CrMo4 42CrMo4 4140 SCM440 42CrMo4 42CrMo

 

Chemical Composition(JIS G4051)

C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Mo(%) Ni(%) Cu(%)
0.38-0.43 0.15-0.35 0.6-0.85 0≦0.03 0≦0.03 0.9-1.2 0.15-0.3 0≦0.25 0≦0.3

 

Introduce

SCM440 is medium carbon chromium molybdenum alloy steel, which is an alloy steel containing chromium and molybdenum. It has the advantages of stable composition, low harmful elements, high steel purity, small decarburization layer and few surface defects. It is easy to be spheroidized and has low cold cracking rate. It is usually hardened and tempered. The ultimate tensile strength is 850-1000 Mpa. This material achieves a very good balance between strength, toughness and wear resistance. The chromium content of the alloy provides good hardness permeability, and the molybdenum element imparts average hardness and high strength.

 

SCM440 reacts well in heat treatment and it is easy to process under heat treatment conditions. This material provides many desirable properties such as good strength and wear resistance, excellent toughness, good ductility and resistance to high-temperature stresses.

 

Product Features:

  1. High strength and toughness.
  2. Great property of quenching and can be deep hardened.
  3. Less tempering brittleness tendency.
  4. Great machining performance under high temperature and nice appearance after machining.
  5. Good performance in weld ability.
  6. Excellent performance in impact absorption, such as where the hammer may bounce back and has barely any damage caused upon impact.

 

Conditions of heat treatment

Annealing: 830℃ Furnace Cooling

Normalization: 830~880℃ Air Cooling

Hardening: 830~880℃ Oil Cooling

Tempering: 530~630℃ Rapid Cooling

Criterion for heat treating conditions revise:

Ac: 750~790℃

Ar: 740~690℃

Ms: 310℃

 

Mechanical properties

Tensile strength (kgf/mm²): ≧100

Yield strength (kgf/mm²): ≧85

Elongation (%): ≧12

Cross section reduction rate (%): ≧45

Impact value (J/cm2): ≧6

Hardness (Hb) : 285~352

 

Forming Option

1 Hot rolling process

2 Hot Forging: Electro-hydraulic; High-speed-hydraulic; Oil-hydraulic; Precision-forging

 

Heat-treatment Option

1 +A: Annealed (full/soft/spheroidizing)

2 +N: Normalized

3 +NT: Normalized and tempered

4 +QT: Quenched and tempered (water/oil)

 

Surface Option

1 Black Surface

2 Grounded: Bright but rough ; Not precision

3 Machining for plate: Bright and precision; Little turning scar

4 Peeled/Turned: Bright and precision; Little turning scar

5 Polished: Very Bright and precision size; Not turning scar

 

Other Services

1 Cutting: Small pieces

2 CNC Machine: Produce as your drawing

3 Package: Bare/Nylon/Canvas/Wooden

4 Payment:T/T, L/C, O/A(request credit)

5 Transport:FOB/CFR/CIF/DDU/DDP (train/ship/Air)

 

Mill test certificate

EN 10204/3.1 with all relevant data reg. chem. composition, mech. properties and results of testing.

 

We also supply :

4130 , 4130 p+x , 4140 , 4330v mod , 4340 , 4145h mod , 4317

1.8509 , 1.6523 , 1.7707 , 1.6657 , 1.6587 , 1.6582 , 1.6773

For all products, please check here: Fushun products

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x