41Cr4 (1.7035) is a chromium alloy steel with about 0.40 % carbon, the direct European counterpart of AISI 5140 and JIS SCr440. It hardens through moderate sections and is normally supplied quenched and tempered for shafts, axles and studs.
Equivalent grades
| System | Designation |
|---|---|
| DIN / EN | 41Cr4 — 1.7035 |
| AISI / SAE | 5140 — UNS G51400 |
| JIS | SCr440 (JIS G4105) |
| AFNOR | 38C4 / 42C4 |
Compared with 4140 / 42CrMo4, this grade has no molybdenum: hardenability is lower, so it is chosen for smaller sections where the molybdenum premium buys nothing.
41Cr4 1.7035 SCr440 AISI 5140 Alloy Steel
Grade :41Cr4
Number:1.7035
Classification:Alloy special steel
Our supply size:
Diameter : 80 to 600 mm ;
Length : 1000 to 9000 mm ;
Our advantage:
- High Quality, Reasonable Price
- Over 40 Years Experience
- ISO NQA Certificated Factory
- Worldwide shipping
- Emergency Orders and Fast Delivery
Standard:
EN 10083-3: 2006 Steels for quenching and tempering. alloy steels
EN 10263-4: 2001 Steel rod, bars and wire for cold heading and cold extrusion.steels for quenching and tempering
EN 10250-3: 2000 Open steel die forgings for general engineering purposes. Alloy special steels
EN 10297-1: 2003 Seamless circular steel tubes for mechanical Non-alloy and alloy steel tubes.
Chemical composition % of steel 41Cr4 (1.7035): EN 10083-3-2006
| C | Si | Mn | P | S | Cr |
| 0.38 – 0.45 | Max 0.4 | 0.6 – 0.9 | Max 0.025 | Max 0.035 | 0.9 – 1.2 |
Introduce
DIN41Cr4/1.7035 Steel is one of the most widely used medium carbon quenched and tempered steels in the machinery manufacturing industry as per EN10083 standard.After proper heat treatment, it has good comprehensive mechanical properties, such as good toughness, plasticity and wear resistance, low temperature impact toughness and low notch sensitivity.
Smelting Option
1 EAF: Electric Arc Furnace
2 EAF+LF+VD: Refined-smelting and vacuum degassing
3 EAF+ESR: Electro Slag Remelting
4 EAF+PESR: protective atmosphere Electro Slag Remelting
5 VIM+PESR: Vacuum induction melting
Forming Option
1 Hot rolling process
2 Hot Forging: Electro-hydraulic; High-speed-hydraulic; Oil-hydraulic; Precision-forging
Heat-treatment Option
1 +A: Annealed (full/soft/spheroidizing)
2 +N: Normalized
3 +NT: Normalized and tempered
4 +QT: Quenched and tempered (water/oil)
Surface Option
1 Black Surface
2 Grounded: Bright but rough ; Not precision
3 Machining for plate: Bright and precision; Little turning scar
4 Peeled/Turned: Bright and precision; Little turning scar
5 Polished: Very Bright and precision size; Not turning scar
Other Services
1 Cutting: Small pieces
2 CNC Machine: Produce as your drawing
3 Package: Bare/Nylon/Canvas/Wooden
4 Payment:T/T, L/C, O/A(request credit)
5 Transport:FOB/CFR/CIF/DDU/DDP (train/ship/Air)
Mill test certificate
EN 10204/3.1 with all relevant data reg. chem. composition, mech. properties and results of testing.
We also supply :
4130 , 4130 p+x , 4140 , 4330v mod , 4340 , 4145h mod , 4317
1.8509 , 1.6523 , 1.7707 , 1.6657 , 1.6587 , 1.6582 , 1.6773
For all products, please check here: Fushun products
Related reading
- AISI 4140 / 42CrMo4 — the molybdenum-bearing grade for heavier sections.
- 25CrMo4 / 1.7218 — the lower-carbon member of the same family.
- 42CrMo4 / 1.7225 — higher carbon and molybdenum, for higher strength.
- What is quenching — the cooling step that decides how deep 41Cr4 hardens.