manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

AISI 8630 Alloy Steel

AISI 8630 Alloy Steel

AISI 8630

Our supply size :

Diameter : 80 to 600 mm ;

Length : 1000 to 9000 mm ;

 

Our advantage :

  1. High Quality, Reasonable Price
  2. Over 40 Years Experience
  3. ISO NQA Certificated Factory
  4. Worldwide shipping
  5. Emergency Orders and Fast Delivery

 

CHEMICAL COMPOSITION

Standard Analysis C Si Mn P S Cr Ni Mo
Min 0.28 0.15 0.7 • • 0.4 0.4 0.15
Max 0.33 0.35 0.9 0.035 0.04 0.6 0.7 0.25

 

Modified Analysis C Si Mn P S Cr Ni Mo
Min 0.28 0.15 0.75 • • 0.85 0.7 0.35
Max 0.33 0.35 0.95 0.035 0.04 1 0.9 0.45

 

MECHANICAL PROPERTIES

U.T.S 95 KSI Min
0.2% Proof Stress 75 KSI Min
Elongation 0.17
Red of Area 0.35

 

Introduce

Alloy Steel 8630 offers users good mechanical properties, as well as weldability by most common methods. This popular alloy works well with hot forging and rolling, in addition to annealing.

 

The hardenability limitations of this grade (depth to which it will harden / obtain the specified mechanical properties after heat treatment) must always be taken into account when designing and selecting equipment.

 

Application

Alloy Steel 8630 is utilized for various critical structural parts such as:

Gears

Ring gears

Shafts and crankshafts

Connectors, hangers, and block valves for the oil industry

 

HEAT TREATMENT

Annealing:For optimum machinabilty of this alloy, a microstructure consisting of coarse pearlite and a minimum of ferrite is considered to be optimum. Such a structure can be obtained by austenitizing at 1550ºF (845ºC), furnace cooling to 1350ºF (730ºC) then to 1180ºF (640º) at 20ºF/hr. An alternative is an iso-anneal at 1225ºF (660ºC)

 

Normalizing:1600ºF (870ºC) and air cool.

 

Hardening:The alloy will be austenitized at around 1525 – 1600ºF (830 – 870ºC) and oil or water quenched depending upon section size and intricacy.

 

Tempering:to desired hardness, using temperatures based on past experience, following water or oil quench.

 

Forming Option

1 Hot rolling process

2 Hot Forging: Electro-hydraulic; High-speed-hydraulic; Oil-hydraulic; Precision-forging

 

Heat-treatment Option

1 +A: Annealed (full/soft/spheroidizing)

2 +N: Normalized

3 +NT: Normalized and tempered

4 +QT: Quenched and tempered (water/oil)

 

Surface Option

1 Black Surface

2 Grounded: Bright but rough ; Not precision

3 Machining for plate: Bright and precision; Little turning scar

4 Peeled/Turned: Bright and precision; Little turning scar

5 Polished: Very Bright and precision size; Not turning scar

 

Other Services

1 Cutting: Small pieces

2 CNC Machine: Produce as your drawing

3 Package: Bare/Nylon/Canvas/Wooden

4 Payment:T/T, L/C, O/A(request credit)

5 Transport:FOB/CFR/CIF/DDU/DDP (train/ship/Air)

 

Mill test certificate

EN 10204/3.1 with all relevant data reg. chem. composition, mech. properties and results of testing.

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x