42CrMo4 1.7225 Alloy Steel

42CrMo4 1.7225 Alloy Steel

42CrMo4 1.7225 Alloy Steel

Introduce  

42CrMo4 steel is a low alloy steel containing chromium, molybdenum, and manganese. It is widely used across numerous industries and is an excellent material choice due to its toughness, high fatigue strength, and abrasion and impact resistance. Not many grades can match the versatility and usefulness.

 

Applications   

This alloy finds many applications as forgings for the aerospace and oil and gas industries, along with myriad uses in the automotive, agricultural and defense industries, Typical uses are forged gears and shafts, spindles, fixtures, jigs and collars.

 

Chemical Properties 

C Cr Mn Si Mo S P
0.38-.43% 0.80-1.10% 0.75-1.0% 0.15-0.30% 0.15-0.25% 0-0.040% 0-0.035%

 

Mechanical Properties 

Properties Metric Imperial
Tensile strength 655 MPa 95000 psi
Yield strength 415 MPa 60200 psi
Bulk modulus (typical for steel) 140 GPa 20300 ksi
Shear modulus (typical for steel) 80 GPa 11600 ksi
Elastic modulus 190-210 GPa 27557-30458 ksi
Poisson’s ratio 0.27-0.30 0.27-0.30
Elongation at break (in 50 mm) 25.70% 25.70%
Hardness, Brinell 197 197
Hardness, Knoop (converted from Brinell hardness) 219 219
Hardness, Rockwell B (converted from Brinell hardness) 92 92
Hardness, Rockwell C (converted from Brinell hardness. Value below normal HRC range, for comparison purposes only) 13 13
Hardness, Vickers (converted from Brinell hardness) 207 207
Machinability (based on AISI 1212 as 100 machinability) 65 65

 

Heat Treatment  

42CrMo4 alloy steel is heated at 845°C (1550°F) followed by quenching in oil. Before hardening, it can be normalized by heating it at 913°C (1675°F) for a long period of time, followed by air cooling.

 

Forging

42CrMo4 alloy steel is forged at 926 to 1205°C (1700 to 2200°F)

 

Hot Working 

42CrMo4 alloy steel can be hot worked at 816 to 1038°C (1500 to 1900°F)

 

Cold Working  

42CrMo4 alloy steel can be cold worked using conventional methods in the annealed condition.

 

Annealing 

42CrMo4 alloy steel is annealed at 872°C (1600°F) followed by slowly cooling in the furnace.

 

Tempering  

42CrMo4 alloy steel can be tempered at 205 to 649°C (400 to 1200°F) depending upon the desired hardness level. The hardness of the steel can be increased if it has a lower tempering temperature. For example, a tensile strength of 225 ksi can be achieved by tempering at 316°C (600°F), and tensile strength of 130 ksi can be achieved by tempering at 538°C (1000°F).

 

Hardening  

42CrMo4 alloy steel can be hardened by cold working, or heating and quenching.

 

Machinability  

42CrMo4 alloy steel has good machinability in the annealed condition.

 

We also supply :

4130 , 4130 p+x , 4140 , 4330v mod , 4340 , 4145h mod , 4317

1.8509 , 1.6523 , 1.7707 , 1.6657 , 1.6587 , 1.6582 , 1.6773

For all products, please check here: Fushun products

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x