Nimonic Alloy C-263, N07263, 2.4650

Nimonic Alloy C-263, N07263, 2.4650

Nimonic Alloy C-263, N07263, 2.4650

Brand name

Nimonic C-263, nicrofer 5120 CoTi

Trade name

Alloy C-263

 

Standards

Material No. EN Designation UNS Alloy
2 .4650 NiCr20Cr20MoT N07263 C-263

 

Description

Alloy C-263/2.4650 is a nickel-chromium-cobalt-molybdenum alloy

 

Special properties

Outstanding creep strength up to 850℃. Excellent resistance to oxidation up to 100℃.

 

Chemical Composition

Cr Mo Cu Ni Ti
19.0-21.0 5.60-6.00 ≤0.20 Rest 1.90-2.40
C Si Mn P S
0.04-0.08 ≤0.40 ≤0.60 ≤0.02 ≤0.007
Al Co B
0.30-0.60 19.0-21.0 ≤0.005

 

Mechanical Properties 20℃

0.2% Yield strength Rp

≥N/mm2

Tensile strength Rm

N/mm2

Elongation A5

≥%

Modulus of elasticity

kN/mm2

570 ≥970 30 222

 

Physical Properties 20℃

Density

g/cm3

specific heat capacity

J/kg K

Thermal conductivity W/m K Electrical resistivity

Ω mm2/m

8.4 426 11.7 1.15

 

Suitable welding filler materials

2.4650

 

Application

Parts for gas turbines.

 

Available forms for 2.4650 / ALL0Y C263

Sheets/Plates

Bars

Wire

Tubes/Pipes

Fittings

Forged / cast parts

Finished part (drawing)

 

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x