RA Alloy 333, N06333, 2.4608
Brand name
RA 333
Trade name
Alloy 333
Standards
| Material No. | EN Designation | UNS | Alloy |
| 2 .4608 | NiCr26MoW | N06333 | 333 |
Description
Alloy 333/2.4608 is a nickel-chromium-iron alloy in addition with molybdenum, cobalt, tungsten and silicon.
Special properties
Excellent resistance against oxidation, carbonization and thermal shock. Outstanding high temperature strength up to 1000℃.
Chemical Composition
| Cr | Mo | Cu | Ni | W |
| 24.0-26.0 | 2.50-4.00 | ≤0.50 | 44.0-47.0 | 2.50-4.00 |
| C | Si | Mn | P | S |
| 0.03-0.08 | 0.70-1.50 | 2.00 | ≤0.03 | ≤0.017 |
| Fe | Co | |||
| Rest | 2.50-4.00 |
Mechanical Properties 20℃
| 0.2% Yield strength Rp
≥N/mm2 |
Tensile strength Rm
N/mm2 |
Elongation A5
≥% |
Modulus of elasticity
kN/mm2 |
| 240 | ≥550 | 30 | 201 |
Physical Properties 20℃
| Density
g/cm3 |
specific heat capacity
J/kg K |
Thermal conductivity W/m K | Electrical resistivity
Ω mm2/m |
| 8.2 | 441 | 11.1 | 1.14 |
Suitable welding filler materials
2.4608
Application
Dampers, refractory anchors, refinery flare tips
Available forms for 2.4608 / ALL0Y 333
Sheets/Plates
Bars
Wire
Tubes/Pipes
Fittings
Forged / cast parts
Finished part (drawing)
What RA 333 is for
RA 333 (UNS N06333) is a nickel-iron-chromium alloy with molybdenum, tungsten and a deliberately high silicon content. That combination is aimed at a specific set of furnace problems: carburising atmospheres, oxidising atmospheres, and the two alternating.
The silicon is the unusual part. It improves resistance to carburisation and to sulphur-bearing gases, which is why the alloy appears in muffles, retorts and slag-notch areas rather than in structural components.
Where it is used
- Furnace muffles and retorts in carburising service
- Heat treatment fixtures that cycle between oxidising and reducing
- Slag taps and burner parts where sulphur is present
What to watch
High silicon makes the alloy less forgiving in fabrication: it is harder to weld than 600 or 601, and the weld procedure matters. It is also not a structural alloy at high stress — it is chosen for environment resistance first.
If a part needs both load-carrying capability and carburisation resistance at temperature, the answer is usually a different grade or a redesign, not a heavier section of 333.
Comparing with the other grades
- Alloy 602 CA / 2.4633
- Inconel 617 / 2.4663
- Inconel 690 / N06690
- Inconel 693 / N06693
- Nimonic C-263 / 2.4650
- Inconel against Incoloy — which family to be in at all.
- Heat resistant steel — furnace grades below the nickel alloys.