Alloy 602 CA, N06025, 2.4633
Brand name
Nicrofer 6025 HT
Trade name
Alloy 602 CA
Standards
| Material No. | EN Designation | UNS | Alloy |
| 2 .4633 | NiCr25FeAlY | N06025 | 602 CA |
Description
Alloy 602 CA/2.4633 is a high-carbon nickel-chromium-iron alloy with additions of aluminum and yttrium.
Special properties
Outstanding resistance to oxidation at high temperatures,even under cyclic conditions. Good corrosion resistance in carburizing environments. Excellent high temperature creep properties
Chemical Composition
| Cr | Ti | Cu | Ni | Al |
| 24.0-26.0 | 0.10-0.20 | ≤0.50 | Rest | 1.80-2.40 |
| C | Si | Mn | P | S |
| 0.15-0.25 | 0.50 | 0.50 | ≤0.02 | ≤0.01 |
| Fe | Zr | Y | ||
| 8.00-11.0 | 0.010-0.10 | 0.05-0.12 |
Mechanical Properties 20℃
| 0.2% Yield strength Rp
≥N/mm2 |
Tensile strength Rm
N/mm2 |
Elongation A5
≥% |
Modulus of elasticity
kN/mm2 |
| 270 | ≥670 | 30 | 215 |
Physical Properties 20℃
| Density
g/cm3 |
specific heat capacity
J/kg K |
Thermal conductivity W/m K | Electrical resistivity
Ω mm2/m |
| 7.9 | 450 | 11.3 | 1.15 |
Suitable welding filler materials
2.4649;2.4633
Application
Furnace components, chemical and petrochemical industry
Available forms for 2.4633 / ALL0Y 602 CA
Sheets/Plates
Bars
Wire
Tubes/Pipes
Fittings
Forged / cast parts
Finished part (drawing)

Why 602 CA exists
Most high-temperature nickel alloys rely on a chromia layer for protection, and that layer stops being reliable much above 1000–1050 °C. Alloy 602 CA takes a different route: about 25 % chromium with roughly 2 % aluminium and a small yttrium addition, so the protective layer is alumina rather than chromia.
Alumina is slower to grow and far more stable at temperature. That is what allows continuous service near 1200 °C — and, unusually for an alloy in this class, it also has the creep strength to carry load at that temperature rather than only resist oxidation.
Where it is used
- Furnace rolls and radiant tubes — the load-bearing high-temperature parts where 601 creeps and 602 CA does not.
- Calciners and rotary kilns — where the atmosphere cycles between oxidising and reducing.
- Glass industry tooling — resistance to both oxidation and the aggressive vapours.
- Heat treatment fixtures that have to survive thousands of cycles without distorting.
What to specify
Solution-annealed condition, grain size, and the forming route if the part is bent or welded. 602 CA is a solid-solution alloy, so there is no ageing condition to call up — but the grain size matters, because coarse grains reduce ductility in the heat-affected zone.
It is also a difficult alloy to machine and form. If the component is complex, the fabrication sequence (form, weld, then solution anneal) is worth agreeing with the mill before the material is ordered.
Comparing with the other grades
- Inconel 617 / 2.4663
- Inconel 690 / N06690
- Inconel 693 / N06693
- RA 333 / N06333
- Nimonic C-263 / 2.4650
- Inconel against Incoloy — which family to be in at all.
- Heat resistant steel — the ferritic and austenitic families below the nickel alloys.