SUH31, 4Cr14Ni14W2Mo, 45KH14N14V2M, 45Х14Н14В2М, Heat Resisting Steel

SUH31, 4Cr14Ni14W2Mo, 45KH14N14V2M, 45Х14Н14В2М, Heat Resisting Steel

16NiCrS4 1.5715 Case Hardening Steels

Equivalent steels

USA Japan France England Hungary Poland Czechia China
– JIS AFNOR BS MSZ PN CSN GB
S66009 SUH31 Z35CNWS14-14 331S42 SZ8 4H14N14W2M 17322 4Cr14Ni14W2Mo

 

Chemical composition

C Si Mn Ni S P Cr Mo W
0.4 – 0.5 max 0.8 max 0.7 13 – 15 max 0.02 max 0.035 13 – 15 0.25 – 0.4 2 – 2.8

 

Mechanical properties under Т=20°С

Assortment sв sT d5 y Heat treatment
– MPa MPa % % –
Bar, GOST 5949-75 710 315 20 35 Drawing 810 – 830°С, air,

 

Physical properties

T E 10– 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 2.08 14 8000 815
100 1.96 16 875
200 1.9 17 17 7930 945
300 1.81 19 507 1000
400 1.73 18 20 7840 511 1055
500 1.66 21 523 1098
600 1.57 18 22 7760 528 1142
700 1.49 24 1172
800 1.41 19 7660

 

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x