manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

MARS 190 Alloy Steel Plate

MARS 190

a quenched and high tempered armor steel

MARS 190 has undergone examination for use in vehicle structures such as main battle tanks and armored personnel carriers, as well as for stationary protection applications like buildings, sentry boxes, and observation posts. Additionally, it has been studied for its effectiveness against various types of targets. The adaptability of MARS 190 is noteworthy, as it seamlessly combines ease of workability even in thicker dimensions with favorable ballistic properties against a wide range of ammunitions.

<<MARS 190 DATA SHEET>>

Standards

France NF A 36-800-CLA
Germany TL 2350 – 0000 Hardness G, H, K, L
UK Stan 95-24 Class 1 and 2, Stan 95-13
US MIL DTL 12560 CL 1.2.3

 

Chemical analysis – Weight %

C S P Si Mn Ni Cr Mo V
≤ .30 ≤ .005 ≤ .012 ≤ .4 ≤ 1.20 ≤ 1.8 ≤ 1.5 ≤ .6 ≤ .10

 

Mechanical properties

Plate thickness (t) hardness range (HB) KCV -40 ° Transverse to rolling direction
mm Inch J ft.lbs
≤ 12 ≤ 0.47 352 – 388 ≥ 20 ≥ 15
12 < t ≤ 35 0.47 < t ≤ 1.38 331 – 375 ≥ 24 ≥ 18
35 < t ≤ 60 1.38 < t ≤2.36 302 – 341 ≥ 32 ≥ 24
60 < t ≤ 85 2.36 < t ≤ 3.30 262 – 331 ≥ 36 ≥ 26
85 < t ≤120 3.30 < t ≤ 4. 72 248 – 285 ≥ 56 ≥ 41
120 < t ≤150 4. 72 < t ≤ 6 241 – 277 ≥ 64 ≥ 47

 

Heat treatment

MARS 190 is a quenched and high tempered armour steel (≥500 °C / 930 ° F)

 

Cutting

Standard thermal cutting techniques (oxygas, plasma, laser) can be used without any special precautions (pre or post-heating) for thicknesses up to 75 mm (3”)

 

Forming

MARS 190 can be cold bent – The rough cut edges have to be ground prior to cold forming

Hot forming can be performed according to process or ; nevertheless, consult us before because temperatures vary according to thickness.

  1. Heating at 900/950 °C (1650/1740 ° F), mandatoryto make a new quality treatment including quenching + tempering.
  2. Heating at 450/550 °C (840/1020 ° F) – air coolingafter forming.

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x