1. Introduction and Applications of Alloy 350

Alloy 350, also known by its UNS designation S35000 or the common trade name AM350, is a chromium-nickel-molybdenum stainless steel. It belongs to the family of precipitation-hardening (PH) stainless steels but is distinctively classified as a semi-austenitic grade. This unique classification means that FUSHUN SPECIAL STEEL produces this material to retain an austenitic structure in the annealed condition, allowing for excellent formability, similar to standard 300-series stainless steels. However, it can be transformed into a hard, high-strength martensitic structure through specific heat treatments, such as sub-zero cooling or double aging.

As a premier manufacturer, FUSHUN SPECIAL STEEL utilizes advanced melting technologies to ensure the purity and consistency of Alloy 350. This material is designed for applications requiring a combination of high strength, good corrosion resistance, and the ability to withstand elevated temperatures. It bridges the gap between the formability of austenitic grades and the strength of martensitic grades.

Typical Applications

Due to its versatile properties, S35000 is widely used in critical industries. We supply this material for:

Aerospace Components: Used in jet engine parts, compressor discs, and turbine blades where strength-to-weight ratio is critical.
Industrial Equipment: Ideal for bellows, industrial cutters, pump seals, and valve components requiring corrosion resistance.
Automotive & Energy: Utilized in gas turbine components and flexible couplings.
Precision Instruments: Used in diaphragms and shafts where dimensional stability after heat treatment is manageable.

2. Chemical Composition of S35000

The chemical balance of AM350 is critical to its semi-austenitic nature. At FUSHUN SPECIAL STEEL, we strictly control the composition, particularly the Nitrogen content, which acts as an austenite stabilizer. Below is the typical composition range we adhere to:

Element Min (%) Max (%)
Carbon (C) 0.07 0.11
Manganese (Mn) 0.50 1.25
Silicon (Si) – 0.50
Chromium (Cr) 16.00 17.00
Nickel (Ni) 4.00 5.00
Molybdenum (Mo) 2.50 3.25
Nitrogen (N) 0.07 0.13
Phosphorus (P) – 0.040
Sulfur (S) – 0.030

3. Mechanical Properties

The mechanical properties of Alloy 350 vary significantly depending on the heat treatment condition. In the annealed state, it is relatively soft and formable. After hardening (e.g., SCT 850 condition), it achieves high strength. FUSHUN SPECIAL STEEL guarantees properties that meet international standards.

Condition Tensile Strength (MPa) Yield Strength 0.2% (MPa) Elongation (%) Hardness (HRC)
Annealed ~ 1100 Max ~ 415 30 Min Max 30 HRC
SCT 850 (Hardened) 1310 Min 1035 Min 10 Min 45-50 HRC

*Note: SCT 850 involves Sub-Zero Cooling and Tempering. Mechanical values are typical and can be customized based on specific client requirements.

4. Heat Treatment of AM350

Proper heat treatment is essential to unlock the potential of Alloy 350. As a fully integrated manufacturer, FUSHUN SPECIAL STEEL provides materials in the annealed condition or heat-treated to your specifications.

Annealing

Typically performed at 1065°C (1950°F) followed by rapid cooling. This retains the austenitic structure for forming.

Hardening Methods

Sub-Zero Cooling & Tempering (SCT):

This method involves cooling the material to -73°C (-100°F) to trigger the martensitic transformation, followed by tempering at 455°C (850°F) or higher to achieve desired hardness and ductility.

Double Aging (DA):

An alternative method involving a two-step aging process, typically used when sub-zero facilities are not available, though SCT usually provides superior properties.

5. Equivalent Grades and Standards

We manufacture Alloy 350 to meet various international standards. While it is primarily known by its US designations, we ensure compliance with global specifications.

Region / Standard Grade / Designation
USA (UNS) S35000
USA (Common Name) AM 350 / Alloy 350
USA (AMS) AMS 5548, AMS 5554, AMS 5745
USA (ASTM) ASTM A693 (Type 633)

6. Supply Forms and Dimensions

FUSHUN SPECIAL STEEL is equipped to produce Alloy 350 in various forms through Hot Rolling or Hot Forging processes. We cater to large-scale industrial requirements and bulk orders.

Available Shapes

  • Round Bars
  • Flat Bars
  • Plates / Sheets
  • Wire / Coil

Size Range

  • Round Bar: Dia 10mm – 800mm
  • Flat/Plate: Thickness 10mm – 500mm, Width up to 800mm
  • Forged Blocks: Custom dimensions available
  • Custom Sizes: We welcome inquiries for non-standard dimensions.

We specialize in bulk manufacturing. If you have specific dimensional requirements or large tonnage needs, please contact us directly.

7. Why Choose FUSHUN SPECIAL STEEL?

As a leading manufacturer, we control every step of the production process to ensure the highest quality for our Alloy 350 products. Here are our key advantages:

Premium Smelting Technology

We utilize Electro-Slag Remelting (ESR), Vacuum Induction Melting (VIM), and Vacuum Arc Remelting (VAR) technologies. This ensures high purity, low gas content, and superior microstructure for high-end aerospace and industrial applications.

In-House Heat Treatment

Our facility is equipped with advanced heat treatment furnaces. We perform annealing, sub-zero cooling, and aging in-house. This guarantees stable mechanical properties, consistent quality control, and faster delivery times.

Machining Capabilities

Beyond raw material production, we offer value-added services including turning, peeling, and grinding. We can deliver “bright bars” or pre-machined components, saving our downstream customers significant time and processing costs.

Manufacturer Direct

Buying directly from FUSHUN SPECIAL STEEL means no middlemen. We welcome large-volume orders and can provide competitive factory-direct pricing with full material traceability.

Ready to Order Alloy 350 / S35000?

Contact FUSHUN SPECIAL STEEL today for quotes on high-quality stainless steel. We are ready to fulfill your bulk requirements.

Contact Us Now

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x