AS 1444 is the Australian standard for wrought alloy steels, including the H-series hardenability grades and hardened and tempered material. It is the specification behind most alloy steel ordered into Australian mining, rail and oil and gas projects.
What the standard provides
- Grade designations and chemical ranges for the common alloy steels
- An H-series — hardenability-controlled grades, analogous to the AISI “H” suffix
- Mechanical property requirements for hardened and tempered supply
- Test frequencies and certificate requirements
The H-series is the part that matters most in practice. It is what allows a buyer to specify that a 4140-type steel must harden to a given depth, rather than hoping the chemistry delivers it.
AS 1444 against AISI and EN
The grades map closely onto the American and European families — the 4140, 4340 and 8620 equivalents are all there — but the specified ranges are not identical, and the hardenability limits in the H-series are set for Australian practice. A drawing written to AS 1444 should be quoted to AS 1444; substituting an AISI grade “because it is the same” is the routine source of argument.
Where it is used
Mining equipment, rail components, pressure equipment and general engineering in Australia and in projects that specify Australian standards abroad. For export orders the same parts often carry a dual citation — AS 1444 plus an ASTM or EN equivalent — and the mill certifies to the more demanding of the two.
What to put on the order
- Grade designation and whether the H-series applies
- Condition: annealed for machining, or hardened and tempered
- Mechanical property requirements, if the part is supplied Q&T
- Whether an equivalent ASTM or EN grade is also acceptable, and if so which one governs
Download the standard
AS 1444 — Wrought alloy steels, standard hardenability H series and hardened and tempered (PDF)
Related reading
- ASTM A304 — the American hardenability-band specification.
- AISI 4140 — the grade most often cited in the H-series.
- Standards library — the full index.