ASTM A304 2004 Standard Specification for Carbon and Alloy Steel Bars Subject to End Quench Hardenability Requirements

ASTM A304 specifies carbon and alloy steel bars by hardenability rather than by chemistry alone. It is the standard behind the “H” suffix — 4140H, 4340H, 8620H — and it exists because two heats with identical analysis can harden to different depths.

What the specification actually controls

Chemistry sets the range; hardenability sets the performance. A304 calls up the end-quench test (ASTM A255) and writes limits on the hardness at defined distances from the quenched end of the specimen — J1.5, J5, J9 and so on, in sixteenths of an inch.

A buyer specifying 4140H is asking for a hardenability band, not just a composition. That is what makes the steel predictable in a part whose section size varies.

Why it matters in practice

  • Section size — a part with a thick hub and a thin flange needs a steel that hardens through both; chemistry alone does not guarantee it.
  • Heat-to-heat consistency — the band removes the case where one heat of 4140 hardens through and the next does not.
  • Cost — tighter hardenability bands cost more, because the mill has to select and verify heats rather than ship to a composition range.

How the H grades are written

The base grade keeps its number and gains an H: 4140 becomes 4140H, 8620 becomes 8620H. The hardenability limits for each are tabulated in A304, and the mill certificate states the actual J values so the buyer can check them against the band.

Where it is used

Gears, shafts, bolts and any quenched and tempered part whose section varies, particularly in the automotive and off-highway supply chain where the heat treatment is fixed and the steel has to be consistent.

Download the standard

ASTM A304 — Carbon and Alloy Steel Bars Subject to End-Quench Hardenability Requirements (PDF)

Related reading

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x