manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

CoCrMo (F75) Master Alloy Ingot for Implant Casting

Master alloy · Cobalt-chrome · ASTM F75 / Stellite 21

CoCrMo Master Alloy for Dental and Orthopaedic Casting

Small volume, long relationship. A dental or orthopaedic casting house that qualifies a CoCrMo heat does not change supplier for a decade, so the sale is decided by documents rather than by cost per kilogram. We supply 3–25 kg ingots to ASTM F75, with nickel held under 0.50 %, full lot traceability and the material-side file that ISO 10993 work starts from.

3–25 kg
Ingot weight
Ni ≤0.50 %
ASTM F75 limit
27–30 %
Chromium
EN 10204 3.1
With trace elements

At a glance

Item CoCrMo master alloy
Designation CoCrMo · ASTM F75 · ISO 5832-4 · Stellite 21 family
Form Cast ingot 3 / 5 / 10 / 25 kg; cut pieces on request
Condition As cast, blasted; surface cleaned for casting
Melting route VIM; VIM+ESR for larger orthopaedic lots
Standards ASTM F75 · ISO 5832-4 · ISO 10993 file support
Certificate EN 10204 3.1, chemistry including Ni, Fe, C and trace elements

Two markets buy this grade and they behave differently. Dental labs cast small batches and care about castability and surface finish. Orthopaedic houses run qualified processes and care about batch consistency, nickel content and paperwork that survives an audit. The ingot is the same; the specification and the file around it are not.

What is different here

CoCrMo is not sold on strength. It is sold on the fact that the material will still be the same material in ten years, and on the fact that the file will satisfy a notified body. Three things follow from that.

  • Chemistry stability, not chemistry range — carbon at 0.20 % and at 0.30 % are both inside ASTM F75 and give different carbide structures and different polishability. We hold an aim value and report it heat by heat.
  • Nickel under control — the F75 limit is 0.50 % and allergy-sensitive patients are the reason. Every heat is reported, not every batch.
  • Documentation as a deliverable — chemistry, gas, trace elements, heat number, and a material file that the customer’s ISO 10993 work can reference.

What we do not do is claim the implant is biocompatible. Biocompatibility is established on the finished device, by the device maker, through ISO 10993 testing. Our job is to make the material side of that file complete and repeatable — and to say so plainly, because a supplier who promises the certificate is a supplier who does not understand it.

Document chain behind a CoCrMo medical casting
The document chain behind a medical casting: each step carries the heat number forward, and the material file is assembled from the melt record rather than reconstructed at the end.

Supply forms and sizes

Form Size Length Tolerance Surface Fits
Ingot 3 / 5 / 10 / 25 kg — Per mould As cast, blasted Dental and orthopaedic crucibles
Cut ingot From 10 / 25 kg Per charge ±2 mm Sawn, cleaned One charge per lot
Round bar Ø30–100 mm 200–1,000 mm ±1 mm Turned Remelt and machining stock

For a dental lab the 3 kg ingot is the practical unit: it matches a small crucible and it keeps the heat number intact across a week of casting. For an orthopaedic lot the 25 kg ingot is cut to charge weight and the cut face is cleaned, because a saw-cut face with coolant residue is the most common source of porosity in the first casting of a lot.

Chemical composition

Element, % ASTM F75 ISO 5832-4
Co Balance Balance
Cr 27.0–30.0 26.5–30.0
Mo 5.0–7.0 4.5–7.0
Ni ≤0.50 ≤0.50
Fe ≤0.75 ≤0.75
C ≤0.35 ≤0.35
Si ≤1.00 ≤1.00
Mn ≤1.00 ≤1.00
P / S ≤0.020 / ≤0.010 ≤0.020 / ≤0.010
N ≤0.25 ≤0.25

The two standards are close but not identical, and the differences sit at the edges of the window rather than in the middle. If the drawing cites ISO 5832-4, quote against it: chromium from 26.5 %, molybdenum from 4.5 %, and the castability changes with both.

Gas content and cleanliness

Item Medical casting grade Industrial grade
Oxygen ≤50 ppm ≤80 ppm
Nitrogen ≤80 ppm ≤120 ppm
Carbon Aim value held, 0.20–0.30 % typical Within F75 range
Trace elements Reported per heat, Cd and Be not intentionally added On request
Inclusion Metallographic report, agreed scale Visual

Oxygen in a cobalt-chrome melt comes from the crucible and the charge, and it shows up as oxide inclusions that blunt a burr and spoil a polished surface. For dental work that is the defect the lab notices first, before any mechanical property.

Mechanical acceptance

Property ASTM F75 requirement Measured on
Tensile strength ≥655 MPa Cast-to-shape test bar
0.2 % yield ≥450 MPa Cast-to-shape test bar
Elongation ≥8 % In 50 mm
Hardness 25–35 HRC typical Cast and polished section
Elastic modulus 210–253 GPa Reference value

F75 properties are casting properties. They are demonstrated on bars cast from the same heat under the qualified process, not on the ingot, and the carbon level is what moves hardness and elongation in opposite directions. A heat that meets the chemistry and misses the elongation is almost always a carbon or a cooling-rate story.

Standards and the documentation file

  • ASTM F75 — cast CoCrMo for surgical implants, chemistry and properties
  • ISO 5832-4 — the ISO counterpart, used across Europe
  • ISO 10993 — biocompatibility of the finished device; we supply the material-side data, the device maker runs the tests
  • EN 10204 3.1 — inspection certificate with the heat number
  • Stellite 21 — the wear-grade trade name customers often quote; same family, different carbon and application

If a customer asks whether F75 and Stellite 21 can be used interchangeably, the answer is no, and the reason is carbon. F75 caps carbon at 0.35 % for implant castings; the wear-grade cobalt alloys run higher carbon for hardness. Quoting one against the other is how a supplier loses a medical account in the first order.

Packing, marking and traceability

  • Ingot — grade, heat number, weight and melt date stamped or tagged
  • MTC — chemistry including Ni, Fe, C and trace elements, standard applied, inspector and date
  • Packing — individual wrap, crate, desiccant; no wooden contact with the ingot face
  • Retention — heat file retained so a repeat order can be matched to the original heat

What to send with an enquiry

Send these five lines and we quote within one working day
  • Standard — ASTM F75 or ISO 5832-4, and the drawing that cites it
  • Application — dental, orthopaedic, or wear part; it decides the carbon aim
  • Ingot weight and quantity per lot
  • Nickel and trace-element limits, plus the documentation package required
  • Certificate and delivery terms — 3.1 as standard, third-party testing at cost

Email [email protected]  ·  WhatsApp +86 178 7358 1838  ·  or use the form below.

FUSHUN METAL · AS9120B · EN 10204 3.1 with the heat number.

Related grades and reading

Cobalt-base and nickel-base alloys used in the same casting shops.

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x