Duplex Stainless Forgings

1. Specifications & Capability

FUSHUN METAL forges duplex and super duplex stainless components in F51 (S31803/2205, 1.4462) and F53 (S32750/2507, 1.4410), solution annealed and compliant with NACE MR0175 for sour service. These are the valve bodies, fittings and flanges of offshore and sour oil and gas fields.

The duplex microstructure – roughly equal parts austenite and ferrite – combines the strength of ferrite with the corrosion resistance of austenite, giving roughly twice the yield strength of a standard austenitic stainless.

Grade Standard Type
F51 / 2205 / 1.4462 ASTM A182 Duplex stainless
F53 / 2507 / 1.4410 ASTM A182 Super duplex stainless

2. Components & Service Conditions

These forgings are the valve bodies, fittings and flanges of offshore platforms and sour oil and gas fields, where the service combines chloride-bearing seawater or brine with hydrogen sulfide. Under these conditions ordinary stainless steels suffer pitting and chloride stress-corrosion cracking, and carbon steels fail by sulfide stress cracking.

The duplex grades resist both mechanisms: the ferrite gives resistance to chloride stress-corrosion cracking, and the chromium, molybdenum and nitrogen give pitting resistance – the super duplex F53, with higher chromium, molybdenum and nitrogen, is specified for the most aggressive sour and chloride environments. Solution annealing develops the correct austenite-ferrite balance, and corrosion testing confirms resistance to the service medium.

3. Grade Equivalents – F51 (2205) / F53 (2507)

Designation Standard Notes
F51 / S31803 / 2205 / 1.4462 ASTM A182 Standard duplex
F53 / S32750 / 2507 / 1.4410 ASTM A182 Super duplex
S32205 / 2205 ASTM A182 Higher-nitrogen duplex variant
00Cr22Ni5Mo3N GB/T 1220 Reference only, not used in certification
F51 duplex stainless forging
F51 duplex stainless forging
Grade C Cr Ni Mo N
F51 (2205) 0.030 max 21.0-23.0 4.5-6.5 2.5-3.5 0.08-0.20
F53 (2507) 0.030 max 24.0-26.0 6.0-8.0 3.0-5.0 0.24-0.32

The higher chromium, molybdenum and nitrogen of the super duplex F53 give superior pitting resistance, measured by a higher pitting resistance equivalent number.

4. Manufacturing Process

Melting. FUSHUN METAL melts to tight chemistry limits, keeping carbon low and controlling nitrogen, which stabilises the austenite.

Forging. Components are forged with controlled deformation and temperature to develop the correct austenite-ferrite balance.

Solution annealing. The forging is solution annealed and quenched to set the duplex structure and restore corrosion resistance.

Testing. UT, ferrite measurement, mechanical and corrosion tests to NACE MR0175, with full traceability.

5. Standards & Certification

Duplex forgings are supplied to ASTM A182 and compliant with NACE MR0175 / ISO 15156 for sour service, with inspection certificates under EN 10204 3.1. FUSHUN METAL holds ISO 9001 and AS9120B certification.

Related forging: low-temperature forgings.

6. Typical Applications

Offshore platforms

Valve bodies and fittings for offshore topsides.

Sour oil and gas

NACE-compliant forgings for sour service.

Seawater systems

Forgings for seawater and brine handling.

Subsea equipment

Super duplex forgings for subsea manifolds and trees.

7. Inquiry Essentials

To quote your duplex forging, please provide the component drawing, the service medium, and the required grade (F51 or F53).

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.