manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

Heat Exchanger Tubesheet Forgings

1. Specifications & Capability

FUSHUN METAL forges heat exchanger tubesheets in F22, F304 and F316, up to 3000 mm diameter, for refinery, nuclear and chemical exchangers. Tubesheets are forged as single pieces, then drilled and prepared for strength expansion of the tubes.

Forging the tubesheet from a single piece gives through-thickness uniformity – the critical requirement for the densely drilled plate that separates shell-side and tube-side fluids.

Grade Standard Diameter
F22 ASTM A336 Up to 3000 mm
F304 / F316 ASTM A182 Up to 3000 mm

2. Components & Service Conditions

The tubesheet is the thick, densely drilled plate that separates the shell-side from the tube-side fluid in a heat exchanger, with hundreds or thousands of tubes expanded into it. It must withstand the pressure differential across it while the ligament between holes remains structurally sound.

Through-thickness uniformity and freedom from lamination are the controlling requirements, because any internal defect between tube holes weakens the ligament. Forging from a single piece, with the grain oriented through the thickness, gives the homogeneous structure that drilling demands, and full-section ultrasonic testing confirms freedom from lamination before machining. F22 is used for high-temperature refinery service, F304/F316 for corrosion resistance.

3. Grade Equivalents – F22 / F304 / F316

Designation Standard Notes
F22 ASTM A336 2.25Cr-1Mo tubesheet
F304 ASTM A182 Austenitic stainless
F316 ASTM A182 Molybdenum-bearing stainless
13CrMo4-5 / 1.7335 EN 10222 European Cr-Mo equivalent
12Cr2Mo1 GB/T 150 Reference only, not used in certification
F316 heat exchanger tubesheet forging
F316 heat exchanger tubesheet forging
Grade C Mn Cr Ni Mo
F22 0.05-0.15 0.30-0.60 2.00-2.50 0.87-1.13
F316 0.08 max 2.0 max 16.0-18.0 10.0-14.0 2.00-3.00

F22 gives elevated-temperature strength for refinery service; F316’s molybdenum improves corrosion resistance over F304 in chloride-bearing environments.

4. Manufacturing Process

Forging. FUSHUN METAL forges the tubesheet as a single piece, orienting the grain through the thickness for ligament strength.

Heat treatment. F22 is quenched and tempered; F304/F316 are solution annealed.

Drilling & expansion. The tubesheet is drilled and prepared for strength expansion of the tubes, with through-thickness uniformity verified.

Testing. Full-section UT for lamination, mechanical tests, with full traceability and inspection certificates under EN 10204 3.1.

5. Standards & Certification

Tubesheets are supplied to ASTM A336 and EN 10222, with inspection certificates under EN 10204 3.1 and optional 3.2 third-party inspection. FUSHUN METAL holds ISO 9001 and AS9120B certification.

Related forging: nuclear RPV forgings.

6. Typical Applications

Refinery exchangers

F22 tubesheets for refinery heat exchangers.

Nuclear exchangers

Tubesheets for nuclear steam generators and exchangers.

Chemical exchangers

F304/F316 tubesheets for chemical service.

Evaporators

Tubesheets for evaporator and condenser units.

7. Inquiry Essentials

To quote your tubesheet, please provide the tubesheet drawing with tube hole layout, the required grade, and the ultrasonic testing requirements.

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x