manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

Inconel Alloy 690, N06690, 2.4642

Inconel Alloy 690,  N06690,  2.4642

Inconel Alloy 690, N06690, 2.4642

Brand name

INCONEL Alloy 690

 

Trade name

Alloy 690

 

Standards

Material No. EN Designation UNS Alloy
2 .4642 NiCr29Fe N06690 690

 

Description

Alloy 690 / 2.4642 is a nickel-chromium-iron alloy.

 

Special properties

High corrosion resistance to oxidizing media.

 

Chemical Composition

Cr Fe Cu Ni Ti
27.0-31.0 7.00-11.0 ≤0.50 Rest 0.50
C Si Mn P S
0.05 ≤0.50 ≤0.50 ≤0.02 ≤0.015
Al
≤0.50

 

Mechanical Properties 20℃

0.2% Yield strength Rp

≥N/mm2

Tensile strength Rm

N/mm2

Elongation A5

≥%

Modulus of elasticity

kN/mm2

340 586 30 215

 

Physical Properties 20℃

Density

g/cm3

specific heat capacity

J/kg K

Thermal conductivity W/m K Electrical resistivity

Ω mm2/m

8.2 450 12 1.15

 

Suitable welding filler materials

2.4648

 

Application

Nuclear fuel processing, steam generators in pressurized water reactors

 

Available forms for 2.4642 / ALL0Y 690

Sheets/Plates

Bars

Wire

Tubes/Pipes

Fittings

Forged / cast parts

Finished part (drawing)

Why 690 has so much chromium

Inconel 690 carries 27–31 % chromium, which is high even for a nickel alloy. The reason is specific: it was developed to resist corrosive attack in high-purity, high-temperature water, and to resist the sulphur-bearing and oxidising conditions where the lower-chromium 600 grade had failed.

More chromium means a more stable passive film, and that is what makes 690 the standard choice for nuclear steam generator tubing and for nitric acid service.

Where it belongs

  • Nuclear steam generator tubing — the application that drove its development.
  • Nitric acid plant — oxidising acid where high chromium is exactly what is needed.
  • Heat treatment fixtures and furnace parts where both oxidation and carburisation are present.

Where it does not

Reducing acids and chloride-bearing solutions are not its strength. It has high chromium but only modest molybdenum, so in chlorides and in reducing environments a 625 or a C-276 will outperform it. Matching the alloy to the medium matters more than the headline chromium figure.

Comparing with the other grades

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.