ASTM A311 Specification for cold drawn, stress relieved carbon steel bars subject to mechanical property requirements
https://www.fushunspecialsteel.com/wp-content/uploads/2015/09/ASTM-A311-Specification-for-cold-drawn-stress-relieved-carbon-steel-bars-subject-to-mechanical-property-requirements.pdf