manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

Inconel Alloy 617, N06617, 2.4663

Inconel Alloy 617,  N06617,  2.4663

Inconel Alloy 617, N06617, 2.4663

Brand name

INCONEL Alloy 617

 

Trade name

Alloy 617

 

Standards

Material No. EN Designation UNS Alloy
2 .4663 NiCr23Co12Mo N06617 617

 

Description

Alloy 617 / 2.4663 is a nickel-chromium-cobalt-molybdenum alloy.

 

Special properties

Excellent mechanical properties up to 1100℃. Excellent resistance to oxidation up to 1100℃.

 

Chemical Composition

Cr Mo Co Ni Ti
20-23 8.50-10.0 11.0-14.0 Rest 0.20-0.60
C Si Mn P S
0.05-0.10 ≤0.20 ≤0.20 ≤0.01 ≤0.01
B Fe Cu Al
≤0.006 ≤2.00 ≤0.50 0.70-1.40

 

Mechanical Properties 20℃

0.2% Yield strength Rp 2

≥N/mm2

Tensile strength Rm

N/mm2

Elongation A5

≥%

Modulus of elasticity

kN/mm2

300 690 35 212

 

Physical Properties 20℃

Density

g/cm3

specific heat capacity

J/kg K

Thermal conductivity W/m K Electrical resistivity

Ω mm2/m

8.4 420 13.4 1.22

 

Suitable welding filler materials

2.4627; 2.4628

 

Application

Components for gas turbines, petrochemical industry

 

Available forms for 2.4663 / ALL0Y 617

Sheets/Plates

Bars

Wire

Tubes/Pipes

Fittings

Forged / cast parts

Finished part (drawing)

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x