manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

Pump Shaft & Valve Stem Forgings

1. Specifications & Capability

FUSHUN METAL forges pump shafts, valve stems and nitrided shafts in 17-4PH (1.4542 / S17400), PH13-8Mo (S13800) and nitriding steel 41CrAlMo7 (1.8509), 200-500 mm in diameter and up to 12 m long. 17-4PH and PH13-8Mo are precipitation-hardening (PH) stainless steels combining high strength with corrosion resistance; 41CrAlMo7 develops a hard wear-resistant case over a tough core.

The forging ratio is at least 4:1, with the grain flow oriented along the shaft axis for maximum fatigue resistance in rotating service.

Grade / Condition Rm (MPa) Rp0.2 (MPa) A (%) Hardness
17-4PH, H1075 aged 1000 min 860 min 13 31-38 HRC
PH13-8Mo, H1000 aged 1410 min 1310 min 10 44-48 HRC
41CrAlMo7, nitrided 900-1100 700 min 10 900+ HV surface

Values follow ASTM A705, AMS 5629 and EN 10085; the aging or nitriding cycle and target hardness are agreed to the component specification.

2. Components & Service Conditions

FUSHUN METAL forges centrifugal pump shafts, valve stems and nitrided shafts for nuclear pumps, chemical valves and industrial rotating equipment. Service conditions combine high speed, bending stress and corrosive or erosive media.

The precipitation-hardening grades are chosen where corrosion resistance plus strength is required – 17-4PH for general pump service and PH13-8Mo for the highest strength and toughness in demanding aerospace and nuclear applications – while the nitriding steel is used where surface wear resistance matters most. Forging, rather than bar stock, is specified so the grain flow follows the shaft contour and internal defects are eliminated, which is critical in safety-related pump shafts.

3. Grade Equivalents – 17-4PH / PH13-8Mo / 1.8509

Designation Standard Notes
17-4PH / 1.4542 / S17400 ASTM A705 Precipitation-hardening stainless
PH13-8Mo / S13800 AMS 5629 High-strength PH stainless
41CrAlMo7 / 1.8509 EN 10085 Nitriding steel
XM-12 / 15-5PH ASTM A705 Related PH stainless
0Cr17Ni4Cu4Nb GB/T 1220 Reference only, not used in certification
17-4PH pump shaft forging
17-4PH pump shaft forging
Grade C Si Mn Cr Ni Others
17-4PH (1.4542) 0.07 max 1.0 max 1.0 max 15.0-17.5 3.0-5.0 Cu 3.0-5.0, Nb 0.15-0.45
PH13-8Mo (S13800) 0.05 max 0.10 max 0.10 max 12.25-13.25 7.5-8.5 Mo 2.0-2.5, Al 0.90-1.35
41CrAlMo7 (1.8509) 0.38-0.45 0.20-0.50 0.50-0.80 1.50-1.80 – Mo 0.25-0.40, Al 0.80-1.20

PH13-8Mo is an ultra-clean grade with P max 0.010 and S max 0.008 for maximum toughness; its aluminum content enables the high hardening response that gives it strength above 17-4PH.

4. Manufacturing Process

Steelmaking. FUSHUN METAL melts these stainless and nitriding steels in an electric arc furnace with refining and vacuum degassing; PH13-8Mo is produced to ultra-clean limits for maximum toughness.

Forging. Shafts are forged with a minimum 4:1 reduction ratio on a 20/80 MN fast forging press, aligning grain flow with the shaft contour.

Heat treatment. 17-4PH and PH13-8Mo are solution treated and precipitation hardened to the ordered aging condition; 41CrAlMo7 is nitrided to produce a hard wear-resistant surface over a tough core.

Testing. Full-section UT, hardness and hardness-profile verification, with complete heat and process traceability.

5. Standards & Certification

Pump shafts and valve stems are supplied to ASTM A705 (17-4PH forgings), AMS 5629 (PH13-8Mo) and EN 10085 (nitriding steel), with inspection certificates under EN 10204 3.1. FUSHUN METAL holds ISO 9001 and AS9120B certification with complete heat and process traceability.

Related forging: gearbox shafts.

6. Typical Applications

Nuclear pump shafts

PH stainless shafts for primary and auxiliary coolant pumps.

Centrifugal pump shafts

High-strength shafts for industrial and chemical pumps.

Valve stems

Stems for gate, globe and control valves in corrosive service.

Nitrided shafts

41CrAlMo7 shafts with hard wear-resistant nitrided surfaces.

7. Inquiry Essentials

To quote your pump shaft or valve stem, please provide the shaft drawing, the required hardness or aging condition, the corrosion resistance requirement, and the applicable standard.

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]