manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

Wind Turbine Flange Forgings

1. Specifications & Capability

FUSHUN METAL ring-rolls wind turbine flanges – tower, nacelle and blade flanges – in S355J2+N (1.0577) and 42CrMo4 (1.7225), up to 5000 mm outside diameter. Every flange is 100% ultrasonically tested to EN 10228-3.

Ring rolling produces continuous circumferential grain flow and eliminates the weld seam of a fabricated flange, giving the structural integrity and fatigue life a tower connection demands.

Grade Standard Outside Diameter
S355J2+N / 1.0577 EN 10025 3000-5000 mm
42CrMo4 / 1.7225 EN 10250-3 3000-5000 mm

2. Components & Service Conditions

Wind turbine flanges join the tower sections, the tower to the nacelle, and the blades to the hub, carrying both static and fluctuating wind loads over a 20-year design life. The bolted connection is a fatigue-critical detail, so the flange must be sound, flat and free of internal defects.

S355J2+N provides the structural strength with guaranteed low-temperature toughness, while 42CrMo4 is used where a quenched and tempered flange of higher strength is required. Ring rolling removes the weld seam of a fabricated flange and aligns the grain flow circumferentially, and the 100% ultrasonic test confirms freedom from the internal defects that would shorten fatigue life.

3. Grade Equivalents – S355J2+N / 42CrMo4

Designation Standard Notes
S355J2+N / 1.0577 EN 10025 Structural steel, normalized
42CrMo4 / 1.7225 EN 10250-3 QT alloy steel option
A572 Gr.50 ASTM A572 US structural equivalent
Q345E GB/T 1591 Reference only, not used in certification
S355J2 wind turbine flange forging
Wind turbine flange forging
Grade C Si Mn Cr Mo
S355J2+N (1.0577) 0.20 max 0.55 max 1.60 max – –
42CrMo4 (1.7225) 0.38-0.45 0.40 max 0.60-0.90 0.90-1.20 0.15-0.30

The J2 quality guarantees Charpy impact toughness at -20 C, essential for cold-climate and offshore wind towers.

4. Manufacturing Process

Melting. FUSHUN METAL melts in an electric arc furnace with ladle refining for cleanliness and low-temperature toughness.

Ring rolling. The billet is upset, pierced and ring-rolled to the flange outside diameter, producing continuous circumferential grain flow and removing the weld seam.

Heat treatment. S355J2+N is normalized; 42CrMo4 is quenched and tempered.

Testing. 100% UT to EN 10228-3, plus dimensional and mechanical verification, with full traceability.

5. Standards & Certification

Wind turbine flanges are supplied to EN 10025 (S355J2+N) and EN 10250-3 (42CrMo4), with ultrasonic testing to EN 10228-3 and inspection certificates under EN 10204 3.1. FUSHUN METAL holds ISO 9001 and AS9120B certification.

Related forgings: nuclear flange rings, large forged flanges and slewing rings.

6. Typical Applications

Tower flanges

Flanges joining wind turbine tower sections.

Nacelle flanges

Flanges connecting the tower to the nacelle.

Blade flanges

Root flanges for wind turbine blades.

Onshore & offshore

Flanges for onshore and offshore wind farms.

7. Inquiry Essentials

To quote your wind turbine flange, please provide the flange specification table, the required batch quantity, and the ultrasonic testing acceptance level.

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x