manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

1.8550 34CrAlNi7-10 Nitriding Steel

1.8550 34CrAlNi7-10 Nitriding Steel

1.8550 34CrAlNi7-10 Nitriding Steel

Grade :34CrAlNi7-10

Number:1.8550

Classification: Nitriding steel

 

Standard:

EN 10085: 2001 Nitriding steel. Technical delivery conditions

 

Our supply size :

Diameter : 80 to 600 mm ;

Length : 1000 to 9000 mm ;

 

Our advantage :

  1. High Quality, Reasonable Price
  2. Over 40 Years Experience
  3. ISO NQA Certificated Factory
  4. Worldwide shipping
  5. Emergency Orders and Fast Delivery

 

Chemical composition % of steel 34CrAlNi7-10 (1.8550)

C Si Mn Ni P S Cr Mo Al
0.3 – 0.37 max0.4 0.4 – 0.7 0.85 – 1.15 max0.025 max0.035 1.5 – 1.8 0.15 – 0.25 0.8 – 1.2

 

Mechanical properties of grade 1.8550 DIN EN 10085

Proof strength Tensile strength Impact energy Elongation at fracture Reduction in cross section on fracture As-Heat-Treated Condition Brinell hardness (HBW)
Rp0.2 (MPa) Rm (MPa) KV (J) A (%) Z (%)
946 (≥) 311 (≥) 44 31 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 131

 

Introduce

1.8550 is intended for work at elevated temperatures in an environment that requires high sliding properties, corrosion, temperature, abrasion, and fatigue resistance. Steel with the addition of Nickel and Aluminum used in the energy, machinery, and automotive industries for large cross-sections elements in the heat treated condition. The products are used in the manufacture of screws, rods, cylinders, pistons, gears, extruders, and rings, which do not require welding.

 

Heat treatment of 34CrAlNi7-10, 1.8550:

Softening annealing at a temperature of 650 – 700 ℃ Hardening at 870 – 930 ℃ for at least half an hour with cooling in water or oil Tempering at 580 – 700℃ for a minimum of 700 hour Nitriding at a temperature of 480 – 570℃

 

Forming Option

1 Hot rolling process

2 Hot Forging: Electro-hydraulic; High-speed-hydraulic; Oil-hydraulic; Precision-forging

 

Heat-treatment Option

1 +A: Annealed (full/soft/spheroidizing)

2 +N: Normalized

3 +NT: Normalized and tempered

4 +QT: Quenched and tempered (water/oil)

 

Surface Option

1 Black Surface

2 Grounded: Bright but rough ; Not precision

3 Machining for plate: Bright and precision; Little turning scar

4 Peeled/Turned: Bright and precision; Little turning scar

5 Polished: Very Bright and precision size; Not turning scar

 

Other Services

1 Cutting: Small pieces

2 CNC Machine: Produce as your drawing

3 Package: Bare/Nylon/Canvas/Wooden

4 Payment:T/T, L/C, O/A(request credit)

5 Transport:FOB/CFR/CIF/DDU/DDP (train/ship/Air)

 

Mill test certificate

EN 10204/3.1 with all relevant data reg. chem. composition, mech. properties and results of testing.

 

We also supply :

4130 , 4130 p+x , 4140 , 4330v mod , 4340 , 4145h mod , 4317

1.8509 , 1.6523 , 1.7707 , 1.6657 , 1.6587 , 1.6582 , 1.6773

For all products, please check here: Fushun products

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x