manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

42CrMoS4 1.7227 Alloy Steel

42CrMoS4 1.7227 Alloy Steel

42CrMoS4 1.7227 Alloy Steel

Grade :42CrMoS4

Number:1.7227

Classification:Alloy special steel

 

Our supply size:

Diameter : 80 to 600 mm ;

Length : 1000 to 9000 mm ;

 

Our advantage:

  1. High Quality, Reasonable Price
  2. Over 40 Years Experience
  3. ISO NQA Certificated Factory
  4. Worldwide shipping
  5. Emergency Orders and Fast Delivery

 

Standard:

EN 10277-5: 2008 Bright steel products. Steels for quenching and tempering

EN 10083-3: 2006 Steels for quenching and tempering. alloy steels

EN 10263-4: 2001 Steel rod, bars and wire for cold heading and cold extrusion for quenching and tempering

 

Equivalent grades of steel 42CrMoS4 (1.7227)

EU Germany France Italy Spain Inter
EN DIN,WNr AFNOR UNI UNE ISO
42CrMoS4 42CrMoS4 42CD4u 42CrMo4 40CrMo41 42CrMoS4

 

Chemical composition % of steel 42CrMoS4 (1.7227):  EN 10277-5-2008

C Si Mn P S Cr Mo
0.38 – 0.45 max   0.4 0.6 – 0.9 max   0.025 0.02 – 0.04 0.9 – 1.2 0.15 – 0.3

 

Mechanical properties of steel 42CrMoS4 (1.7227)

Nominal diameter (mm): to 16 16 – 40 40 – 100 100 – 160 160 – 250
Rm – Tensile strength (MPa) (+QT) 1100-1300 1000-1200 900-1100 800-950 750-900

 

Introduce

42CrMoS4 is a direct hardening steel like 42CrMo4 but with controlled sulphur content for improved machinability. The material is stocked in cold drawn hardened and tempered condition.

 

APPLICATION

42CrMoS4 has high strength and wear-resistance,widely used in many industries.

Components with high strength and toughness for tools, automotive parts,mechanical engineering, armament components,such as geer wheels,pinions,connecting rods,parts for mechanical engineering.

Statically and dynamically stressed components for vehicles, engines and machines. For parts of larger cross-sections, crankshafts,gears

 

Smelting Option

1 EAF: Electric Arc Furnace

2 EAF+LF+VD: Refined-smelting and vacuum degassing

3 EAF+ESR: Electro Slag Remelting

4 EAF+PESR: protective atmosphere Electro Slag Remelting

5 VIM+PESR: Vacuum induction melting

 

Forming Option

1 Hot rolling process

2 Hot Forging: Electro-hydraulic; High-speed-hydraulic; Oil-hydraulic; Precision-forging

 

Heat-treatment Option

1 +A: Annealed (full/soft/spheroidizing)

2 +N: Normalized

3 +NT: Normalized and tempered

4 +QT: Quenched and tempered (water/oil)

 

Surface Option

1 Black Surface

2 Grounded: Bright but rough ; Not precision

3 Machining for plate: Bright and precision; Little turning scar

4 Peeled/Turned: Bright and precision; Little turning scar

5 Polished: Very Bright and precision size; Not turning scar

 

Other Services

1 Cutting: Small pieces

2 CNC Machine: Produce as your drawing

3 Package: Bare/Nylon/Canvas/Wooden

4 Payment:T/T, L/C, O/A(request credit)

5 Transport:FOB/CFR/CIF/DDU/DDP (train/ship/Air)

 

Mill test certificate

EN 10204/3.1 with all relevant data reg. chem. composition, mech. properties and results of testing.

 

We also supply :

4130 , 4130 p+x , 4140 , 4330v mod , 4340 , 4145h mod , 4317

1.8509 , 1.6523 , 1.7707 , 1.6657 , 1.6587 , 1.6582 , 1.6773

For all products, please check here: Fushun products

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.