manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

Archive for the Standards Category

DIN50602 Microscopic examination of special steels using standard diagrams to assess the content of non-metallic inclusions

DIN50602 Microscopic examination of special steels using standard diagrams to assess the content of non-metallic inclusions

Read more →

ASTM E45 2011 Standard Test Methods for Determining the Inclusion Content of Steel

ASTM E45 2011 Standard Test Methods for Determining the Inclusion Content of Steel

Read more →

ASTM A331 1995 Standard Specification for Cold Finished Alloy Steel Bars

ASTM A331 1995 Standard Specification for Cold Finished Alloy Steel Bars

Read more →

ASTM A682 2002 Standard Specification for Steel Strip, High Carbon, Cold Rolled, General Requirements

ASTM A682 2002 Standard Specification for Steel Strip, High Carbon, Cold Rolled, General Requirements

Read more →

ASTM A705 Standard Specification for Age Hardening Stainless Steel Forgings

ASTM A705 Standard Specification for Age Hardening Stainless Steel Forgings

Read more →

ASTM E112 2010 Standard Test Methods for Determining Average Grain Size

ASTM E112 2010 Standard Test Methods for Determining Average Grain Size

Read more →

ASTM A580 2006 Standard Specification for Stainless Steel Wire

ASTM A580 2006 Standard Specification for Stainless Steel Wire

Read more →

ASTM A388 Standard Practice for Ultrasonic Examination of Heavy Steel Forgings

ASTM A388 Standard Practice for Ultrasonic Examination of Heavy Steel Forgings

Read more →

ASTM A311 Specification for cold drawn, stress relieved carbon steel bars subject to mechanical property requirements

ASTM A311 Specification for cold drawn, stress relieved carbon steel bars subject to mechanical property requirements https://www.fushunspecialsteel.com/wp-content/uploads/2015/09/ASTM-A311-Specification-for-cold-drawn-stress-relieved-carbon-steel-bars-subject-to-mechanical-property-requirements.pdf

Read more →

ASTM A304 2004 Standard Specification for Carbon and Alloy Steel Bars Subject to End Quench Hardenability Requirements

ASTM A304 2004 Standard Specification for Carbon and Alloy Steel Bars Subject to End Quench Hardenability Requirements

Read more →

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x