This week we delivered 34CrNiMo6 and 42CrMo4 to Shanghai port for our Swedish clients!

The size of we produced: 51.2mm and 95 mm diameter alloy steel round bar with bright surface!

 

What is 34CrNiMo6?

EN 34CrNiMo6 Steel is an important alloy engineering steel grade as per BS EN 10083-3:2006. 34CrNim06 steel has high strength, high toughness and good hardenability. EN / DIN 34CrNiMo6 alloy steel has the stability of resistance to overheating, but the white sensitivity of 34CrNiM06 is high. It also has the temper brittleness, so the weldability of 34CrNiMo6 material is poor. The steel 34CrNiMo6 needs the high temperature preheating before welding in order to eliminate the stress after welding processing.

 

34CrNiMo6 Chemical Composition

C Mn Si P S Cr Mo Ni
0.30-0.38 0.5-0.8 0.40 max 0.025 max 0.035 max 1.3-1.7 0.15-0.30 1.3-1.7

 

What is 42CrMo4?

42CrMo4 steel it has high strength and toughness, good hardenability, no obvious tempering brittleness, high fatigue limit and multiple impact resistance after quenching and tempering, and good low-temperature impact toughness.

 

42CrMo4 Chemical Composition

C Cr Mn Si Mo S P
0.38-.43% 0.80-1.10% 0.75-1.0% 0.15-0.30% 0.15-0.25% 0-0.040% 0-0.035%

We also supply :

4130 , 4130 p+x , 4140 , 4330v mod , 4340 , 4145h mod , 4317

1.8509 , 1.6523 , 1.7707 , 1.6657 , 1.6587 , 1.6582 , 1.6773

For all products, please check here: Fushun products

 

Fushun Special Steel LTD CO

Fushun Metal is a large special steel manufacturer and supplier. We are metal experts and have been providing quality customer service and products since 1998.

 

At Fushun Metal, we supply a wide range of metals for a variety of applications. Our products/stock includes: stainless steel, alloy steel, spring steel, tool steel, high speed steel, mould steel, nickel alloy.

 

Our hot rolled and cold rolled steel is available in a wide range of shapes including: bars, tubes, sheets and plates. We can cut metal to your exact specifications.

 

Send your inquiry information to us and get a free quotation today!

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x